Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 145 MPa | 21000 psi | ASTM D638 |
Custom Resins Vexel™ E20GF30 , 30% Glass Reinforced PET
(discontinued **) Description: Vexel™ E20GF30 is a 30% glass fiber reinforced, general purpose PET. Information provided by Custom Resins. |
|||
Tensile Strength, Ultimate | 145 MPa | 21000 psi | ASTM D638 |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® BR111BL is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical proper.. |
|||
Tensile Strength, Ultimate | 145 MPa @Temperature 1095 °C |
21000 psi @Temperature 2003 °F |
|
Haynes 188 alloy, hot rolled and 1175°C solution annealed plate Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Ultimate | 145 MPa @Temperature 871 °C |
21000 psi @Temperature 1600 °F |
|
AK Steel 309S Austenitic Stainless steel AK Steel 309S provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic w.. |
|||
Tensile Strength, Ultimate | 145 MPa | 21000 psi | 5mm/min; ISO 527 |
BASF Ultramid® 7523-2AM BK ND3007 33% Glass Filled PA66 (Dry) Ultramid 7523-2AM BK ND3007 is an impact modified, 33% glass reinforced, heat stabilized injection molding PA6/6. |
|||
Tensile Strength, Ultimate | 145 MPa | 21000 psi | 5mm/min; ISO 527 |
BASF Ultramid® 8232G HS FR BK-102 25% Glass Filled PA6 (Dry) Ultramid 8232G HS FR BK-102 is a 25% glass fiber reinforced, heat stabilized, flame retardant pigmented black PA6 injection molding compound exhibiting excellent melt stability characteristics. It .. |
|||
Tensile Strength, Ultimate | 145 MPa | 21000 psi | 5mm/min; ISO 527 |
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry) Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st.. |
|||
Tensile Strength, Ultimate | 145 MPa | 21000 psi | ATSM D638 |
Ashley Polymers Ashlene® 630-25G Nylon 6, 25% Glass Reinforced Nylon 6, 25% glass reinforced resin.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 145 MPa | 21000 psi | ASTM D638 |
Chem Polymer Chemlon 233 GI Nylon 6, 33% Glass Fiber Reinforced A 33% glass fiber reinforced, impact modified nylon 6 offering a combination of creep resistance, stiffness and toughness over unmodified nylon 6 materials.Data provided by the manufacturer, Chem Po.. |
|||
Tensile Strength, Ultimate | 145 MPa | 21000 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 433 Glass Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 145 MPa | 21000 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 610 Nylon 6, Glass/Mineral Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 145 MPa | 21000 psi | ASTM D638 |
A. Schulman ComAlloy Voloy® 613 Nylon 6, Glass Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 145 MPa | 21000 psi | 5 mm/min |
Arkema Group Rilsan® AZM 50 NOIR T6LD Nylon 12, 50% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-090,GF50Rigid grade with glass fiber (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid.. |
|||
Tensile Strength, Ultimate | 145 MPa @Temperature 871 °C |
21000 psi @Temperature 1600 °F |
|
AK Steel 309 Austenitic Stainless steel AK Steel 309 provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic wh.. |
|||
Tensile Strength, Ultimate | 145 MPa | 21000 psi | ISO 527-1/-2 |
DSM Arnite® TV4 261 /A PBT-GF30 30% Glass Reinforced |
|||
Tensile Strength, Ultimate | 145 MPa | 21000 psi | Same value from ASTM and ISO tests; 5 mm/min. |
BASF Capron® 8232G HS FR BK-102 25% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8232G HS FR BK-102 is a 25% glass fiber reinforced, heat stabilized, flame retardant pigmented black nylon 6 injection molding compound exhibiting excellent melt stability characteristics. I.. |
|||
Tensile Strength, Ultimate | 145 MPa | 21000 psi | ASTM D638 |
PolyOne Edgetek® NI-30GF/000 Nylon 6/10 - 30% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 145 MPa | 21000 psi | ASTM D638 |
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Tensile Strength, Ultimate | 145 MPa | 21000 psi | 5mm/min; ISO 527 |
BASF Ultramid® 1503-2 NF2004 33% Glass Filled PA66 (Conditioned) Ultramid 1503-2 NF2004 is a 33% glass reinforced, heat stabilized injection molding PA6/6. |