Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 98.1 MPa | 14200 psi | DIN 53455; ASTM D638 |
Kolon KOPET® KP133135 FR-PET Resin
(discontinued **) KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of p.. |
|||
Tensile Strength, Ultimate | 98.0 MPa | 14200 psi | ISO 527 |
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Tensile Strength, Ultimate | 98.0 MPa | 14200 psi | ISO 527 |
LATI LARIL 13 G/20-V1 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Tensile Strength, Ultimate | 97.9 MPa | 14200 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® SF-20GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 98.1 MPa | 14200 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN333G15HI Multi Reinforced Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Tensile Strength, Ultimate | 97.9 MPa @Thickness 3.17 mm |
14200 psi @Thickness 0.125 in |
ASTM D638 |
LG Chemical Lupox® PBT-GP-2156F 15% GFR Flame Retardant PBT General Purpose PBT, 15% Glass Fiber Reinforced, Weather Resistant, Flame Retardant, Non-Bleed. Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Ultimate | 98.1 MPa | 14200 psi | |
Shinil Chemical SHINCON PPS Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Tensile Strength, Ultimate | 98.1 MPa | 14200 psi | |
Shinil Chemical SHINCON PPS-CNT LCD Rack LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b.. |
|||
Tensile Strength, Ultimate | 98.0 MPa | 14200 psi | ASTM D638 |
Tipco Tipcolene® SEB 300 - 30% Chemically Coupled Glass Fiber Polypropylene Homopolymer with High Heat Stability 30% Chemically Coupled Glass Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Ultimate | 98.0 MPa | 14200 psi | ATSM D638 |
Ashley Polymers Ashlene® 126 PBT Polyester, 30% Glass Reinforced General purpose 30% glass reinforcement, natural. Colors will modify properties.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 98.1 MPa | 14200 psi | 5mm/min; ASTM D638 |
Asia International Enterprise (Hong Kong) 30G3F Polybutylene terephthalate, 15% Glass Fiber Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Tensile Strength, Ultimate | 98.0 MPa | 14200 psi | ATSM D638 |
Ashley Polymers Ashlene® 126WO PBT Polyester, 30% Glass Reinforced PBT polyester with 30% glass reinforcement, flame retardant, natural. Colors will modify properties.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 98.0 MPa | 14200 psi | 5mm/min; ISO 527 |
BASF Ultradur S 4090 G4 BK5110 20% Glass Filled PBT Ultradur S 4090 G4 BK5110 is a 20% glass reinforced, pigmented black PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkag.. |
|||
Tensile Strength, Ultimate | 98.1 MPa | 14200 psi | 5mm/min; ASTM D638 |
Asia International Enterprise (Hong Kong) 30G3 Polybutylene terephthalate, 15% Glass Fiber Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |