Material Notes:
SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's patented conductive filler dispersion technology with variety of engineering polymers and their alloys to impart permanent static dissipative to electrically conductive property to thermoplastics. SHINCON contains multiwall carbon nanotube (MWCNT), carbon black (CB), and carbon fiber (CF) as a conductive filler. SHINCON are used in injection molding, film or sheet extrusion for the applications where the desired level of conductivity and unique mechanical property are important. A wide range of the surface resistaivity is obtained by SHINCON formulations for the parts and devices depending upon customer needs and applications.Feature and BenefitsPermanent electro conductivityMaintain the physical properties of base resinNo particulates (CNT product)Lighter weightRecyclabilityEasy processingImproved surfaceCost effectiveGrade/Application: LCD rackInformation Provided by Shinil Chemical Industry Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.84 g/cc
1.84 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 98.1 MPa
14200 psi
Flexural Strength 225.63 MPa
32725 psi
Flexural Modulus 20.6 GPa
2990 ksi
Izod Impact, Notched 0.490 J/cm
0.918 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 275 °C
527 °F
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+7 ohm-cm
2.00e+7 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 290 °C
554 °F