Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 725 MPa @Temperature 538 °C |
105000 psi @Temperature 1000 °F |
|
Kennametal Stellite Stellite® 3 PM with P/M Processing Typical applications include (aerospace) vane plugs, fuel metering pins, spacer bushings, (bearings) ball blanks, race blanks, (valve seat inserts) diesel engine exhaust, fluid valve seats, saw cutt.. |
|||
Tensile Strength, Ultimate | 725 MPa @Temperature 538 °C |
105000 psi @Temperature 1000 °F |
|
Kennametal Stellite Stellite® 98M2 with P/M Processing Adhesive wear test data P/M 0.58 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw.. |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
Materion BrushBronze® 95510 (AMS 4880) Centrifugal Cast 0.250" - 1.0" Information supplied by Brush Wellman Engineered Materials.BrushBronze™ 95510 is an Aluminum-Nickel-Bronze alloy that combines high strength, ductility, and good abrasion resistance under sever.. |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
Materion BrushBronze® 95510 (AMS 4880) Continuous Cast 0.250" - 4.0" Information supplied by Brush Wellman Engineered Materials.BrushBronze™ 95510 is an Aluminum-Nickel-Bronze alloy that combines high strength, ductility, and good abrasion resistance under sever.. |
|||
Tensile Strength, Ultimate | >= 724 MPa | >= 105000 psi | |
Materion ToughMet® T2 CX 90 ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Tensile Strength, Ultimate | 725 MPa @Temperature 650 °C |
105000 psi @Temperature 1200 °F |
|
Haynes 25 alloy, hot rolled and 1230°C solution annealed sheet Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Ultimate | 725 MPa | 105000 psi | |
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Tensile Strength, Ultimate | 725 MPa | 105000 psi | |
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
Materion BrushBronze® 630 (AMS 4640) 2.0" - 3.0" Information supplied by Brush Wellman Engineered Materials.BrushBronze™ 630 is an Aluminum-Nickel-Bronze alloy that combines high strength along with resistance to wear under severe loading con.. |
|||
Tensile Strength, Ultimate | 725 MPa @Temperature 760 °C |
105000 psi @Temperature 1400 °F |
|
Haynes 263® alloy, cold rolled sheet, solution treated and aged Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle.. |
|||
Tensile Strength, Ultimate | 724 MPa @Temperature 93.0 °C |
105000 psi @Temperature 199 °F |
|
Haynes Hastelloy® C-22® alloy, 12.7-50.8 mm thick bar, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
Special Metals INCONEL® 690 Nickel Superalloy, Cold Rolled Strip, 0.150 inch (3.81 mm) Thick Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and.. |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
Schmolz + Bickenbach MoldMAX® SC Copper Alloy Description: Brush Wellman’s MoldMAX® SC is a high conductivity copper mold alloy with good strength. MoldMAX® SC is used as blow mold cavities, injection mold cores and cavities and hot .. |
|||
Tensile Strength, Ultimate | 725 MPa | 105000 psi | Typical |
TIMET 100A CP Titanium Industry Specifications: USA Aerospace: AMS 4921. Germany Engineering: 3.7065. Germany Aerospace: 3.7064. France: T-60. UK Aerospace Specifications BS TA. 7, 8, 9.Features: The mechanical prope.. |
|||
Tensile Strength, Ultimate | 724 - 820 MPa | 105000 - 119000 psi | |
Eagle Brass 521 Phosphor Bronzes 8% C, Spring Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
Crucible Steel 440A Chromium Steel Crucible 440A is a hardenable chromium steel which is the toughest of the high chromium cutlery grades. This grade is magnetic at all times. Information provided by Crucible Specialty Metals. |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
ATI Allvac® Allcorr® UNS N06110 Nickel Superalloy Uses: Equipment for deep sour gas wells, flue gas desulfurization, chemical and hydrocarbon processing, and pulp and paper.Property values are for samples in the metallurgical condition: 2050°F ann.. |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
ATI Allvac® Vasco® 316-L Specialty Steel, Heat Treatment: 1038°C (1900°F) Anneal Data provided by Allvac.Applications: Jet engine components, exhaust manifold heat exchangers, chemical process equipment, semiconductor systems. |
|||
Tensile Strength, Ultimate | 724 MPa @Temperature 93.0 °C |
105000 psi @Temperature 199 °F |
|
Carpenter Gall-Tough® Stainless Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1.. |
|||
Tensile Strength, Ultimate | 725 MPa | 105000 psi | |
ATI Allegheny Ludlum AL 2003™ Duplex Stainless Steel Characteristics: superior stress corrosion cracking resistance to Types 316 and 317, yield strength double that of conventional austenitic stainless steel, good corrosion resistance, good chloride s.. |