| Category | Metal , Ferrous Metal , Stainless Steel , T 400 Series Stainless Steel |
| Manufacturer | Crucible Steel |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Crucible Steel 440A Chromium Steel.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 7.75 g/cc | 7.75 g/cc |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Brinell | 215 | 215 | |
| Hardness, Rockwell C | 44 | 44 | tempering temperature-1000°F |
| 57 | 57 | as quenched | |
| 57 | 57 | tempering temperature- 212°F | |
| Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
| Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
|
| Elongation at Break | 20 % | 20 % | in 2" |
| Reduction of Area | 45 % | 45 % | |
| Modulus of Elasticity | 200 GPa | 29000 ksi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 10.3 µm/m-°C @Temperature -17.8 - 93.3 °C |
5.70 µin/in-°F @Temperature 0.000 - 200 °F |
|
| 10.8 µm/m-°C @Temperature -17.8 - 316 °C |
6.00 µin/in-°F @Temperature 0.000 - 600 °F |
||
| Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
| Thermal Conductivity | 24.2 W/m-K @Temperature 93.3 °C |
168 BTU-in/hr-ft²-°F @Temperature 200 °F |
|
| Melting Point | 1370 - 1510 °C | 2500 - 2750 °F | |
| Solidus | 1370 °C | 2500 °F | |
| Liquidus | 1510 °C | 2750 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Carbon, C | 0.60 - 0.75 % | 0.60 - 0.75 % | |
| Chromium, Cr | 16 - 18 % | 16 - 18 % | |
| Iron, Fe | >= 78.43 % | >= 78.43 % | As Remainder |
| Manganese, Mn | <= 1.0 % | <= 1.0 % | |
| Molybdenum, Mo | <= 0.75 % | <= 0.75 % | |
| Phosphorous, P | <= 0.040 % | <= 0.040 % | |
| Silicon, Si | <= 1.0 % | <= 1.0 % | |
| Sulfur, S | <= 0.030 % | <= 0.030 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.00005994 ohm-cm @Temperature 23.0 °C |
0.00005994 ohm-cm @Temperature 73.4 °F |