Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
Owens Corning Glass Fiber Reinforced Acrylonitrile Butadiene Styrene (ABS), 20 wt.% glass ABS is highly resistant to weak acids and alkalis, and provides good resistance to most organic solvents. It is attacked by sulfuric and nitric acids, and is soluble in esters, ketones and ethylene .. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® ET-1001 HS Polyphthalamide (PPA) Resin, Dry As Molded
(discontinued **) AMODEL ET-1001 HS resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resist.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
ExxonMobil Escor® AT-320 EMAAA Terpolymer for Polymer Modification
(discontinued **) Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components, such as aluminum foil, polyolefins, polycarbonate, PET, .. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
PolyOne Edgetek® MP-10GF/000 Modified PPO - 10% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 76.0 - 175 MPa | 11000 - 25400 psi | Average value: 132 MPa Grade Count:24 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D882 |
Honeywell Capran® 996 Heat Stabilized Nylon Film
(discontinued **) Description: Capran® 996 is a blue tinted, heat-stabilized cast film produced from modified nylon resin. Capran® 996 has excellent heat stability and resistance to pinholing. It can be used at t.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
IDI Composites E-204 Thermoset Polyester, Sheet ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista.. |
|||
Tensile Strength, Ultimate | 76.0 MPa @Temperature 22.0 °C |
11000 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0900 Unsaturated Polyester UP SMC 0900 is a special SMC for use within a chemical aggressive environment. The glass level is selected to combine good mouldability with good strength and stiffness properties. The product is espec.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | |
Haysite H755 Glass Reinforced Polyester Sheet, Electrical Grade (GPO1) A new generation of IEEE Class F, 155ºC /165ºC NEMA GPO- 1 material. H755 is designed to bridge the gap between 130ºC Class B GPO-1 materials and Class H 180ºC grades. H755 has quickly g.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | |
Haysite Ultratrac® H950 Glass Reinforced Polyester Sheet, Electrical Grade (GPO3) This new generation of high performance material meets or exceeds all requirements for NEMA GPO-2 or GPO-3. ULTRATRAC ® H950 is recognized by U.L. as a 94V-0 material and offers greater arc and t.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
Plenco 00732 Melamine-Phenolic, Granular, Compression Molded PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
Plenco 1586 Polyester, Pellet, Transfer Molded PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injecti.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
Plenco 7556 Phenolic, Briquette, Transfer Molded PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM Data |
Dow Tyril® 880B SAN TYRIL® 880B SAN copolymer combines the high levels of chemical resistance, heat resistance and overall strength of 880 resin with improved mold flow and mold release characteristics.Data provided b.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM Data |
Dow Tyril® 880 SAN TYRIL® 880 SAN copolymer offers excellent physical properties incorporating the highest levels of chemical resistance, heat resistance and overall strength of any TYRIL grade.Data provided by Dow C.. |
|||
Tensile Strength, Ultimate | 76.0 MPa @Temperature 871 °C |
11000 psi @Temperature 1600 °F |
ASTM E8 |
ATI Allegheny Ludlum 310 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | Static |
Channel Industries 5500 Lead Zirconate Titanate Piezoelectric Navy Type IICharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most exten.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | Static |
Channel Industries 5700 Lead Zirconate Titanate Piezoelectric Navy Type VICharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most exten.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 213 Polystyrene, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
A. Schulman ComAlloy Lubrilon® 511 Polycarbonate, Glass Fiber/PTFE, UL Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
A. Schulman ComAlloy Aqualoy® 140 Polypropylene, Glass Reinforced, Chemically Coupled NSF Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
A. Schulman ComAlloy Comtuf® 524 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | Static |
Channel Industries 5400 Lead Zirconate Titanate Piezoelectric Navy Type ICharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most extens.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | Static |
Channel Industries 5600 Lead Zirconate Titanate Piezoelectric Navy Type VCharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most extens.. |