Polymer Property : Tensile Strength, Ultimate = 590 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 590 MPa

@Temperature 100 °C
85600 psi

@Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 2205 Duplex Stainless Steel
Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t..
Tensile Strength, Ultimate 590 MPa
85600 psi
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Ultimate >= 590 MPa
>= 85600 psi
MetalTek H 188 Centri-Vac Nickel Cobalt Based Alloy
Information provided by MetalTek
Tensile Strength, Ultimate >= 590 MPa
>= 85600 psi
Industeel CLC 17.13.5 LN Modified 317LN Mo 4% Austenitic Stainless Steel
Description: CLC 17-13-5LN (317LNM) is a Nitrogen alloyed austenitic stainless steel with a high Molybdenum addition (=4%). Alloy CLC 17-13-5LN (317LNM) exhibits austenitic microstructure free of de..
Tensile Strength, Ultimate >= 590 MPa
>= 85600 psi
Industeel CLC 18.12.4 LN 3%Mo Austenitic Stainless Steel with Nitrogen Addition
Description: CLC 18-12-4LN (317LN) is a Nitrogen alloyed austenitic stainless steel with a 3% Mo minimum addition (>4%). Alloys CLC 18-12-4LN (317LN) exhibit austenitic microstructure free of delete..
Tensile Strength, Ultimate 590 - 725 MPa
85600 - 105000 psi
Materion Brush 1915â„¢ Heat Treated Temper Rod, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe..
Tensile Strength, Ultimate 590 - 725 MPa
85600 - 105000 psi
Materion Brush 1915â„¢ Heat Treated Temper Wire, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee..
Tensile Strength, Ultimate 590 - 770 MPa
85600 - 112000 psi
Typical
Industeel SUPERELSO® 500HR Quenched and Tempered High Strength Steel for Wet H2S Service
Description: Superelso® 500 HR (SE 500 HR, "Hydrogen Resistant") is a 500MPa (72ksi) yield strength quenched and tempered steel adapted for pressure equipment operating under sour service conditi..
Tensile Strength, Ultimate 590 MPa

@Temperature 650 °C
85600 psi

@Temperature 1200 °F
Haynes 556® alloy, cold rolled, solution annealed sheet, 0.8-2.8 mm thick
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Ultimate 590 MPa

@Temperature 550 °C
85600 psi

@Temperature 1020 °F
Annealed prior to test
Special Metals INCOLOY® Alloy 825
A nickel-iron-chromium alloy with additions of molybdenum and copper. It has excellent resistance to both reducing and oxidizing acids, to stress-corrosion cracking, and to localized attack such as..
Tensile Strength, Ultimate 590 MPa

@Temperature 300 °C
85600 psi

@Temperature 572 °F
Annealed prior to test
Special Metals INCOLOY® Alloy MA 956
An iron-chromium-aluminum alloy that is oxide dispersion strengthened and produced by mechanical alloying. Production involves high-energy milling of metal powders to create an alloy with a strengt..
Tensile Strength, Ultimate 590 - 650 MPa
85600 - 94300 psi
Wire
CLAL-MSX ARCAP Anticorrosion AP1 H14 4/4 hard, Drawn Copper Alloy
Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin..
Tensile Strength, Ultimate 590 - 640 MPa
85600 - 92800 psi
T direction
ArcelorMittal Speed 35-440 Electrical Steel
Properties: The iCARe™ Speed product family comes with guaranted losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 590 - 670 MPa
85600 - 97200 psi
ArcelorMittal FB 590 Hot rolled ferrite-bainite steel
Available in the following: uncoated (HDT590F)Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It comprises four strength levels: ..
Tensile Strength, Ultimate 590 MPa

@Temperature 100 °C
85600 psi

@Temperature 212 °F
EN min.; EN 10002-5
Outokumpu LDX 2101® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Tensile Strength, Ultimate 590 - 670 MPa
85600 - 97200 psi
ArcelorMittal FB 590 HHE Hot rolled ferrite-bainite steel
Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It comprises four strength levels: FB 450, 540, 560 and 590. This family of steel..