Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D651
Resinoid 2011 Phenolic Molding, Fabric Reinforced
Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D651
Resinoid 2225 Phenolic Molding, Cellulose Reinforced
Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance
Tensile Strength, Ultimate 53.0 MPa

@Temperature 90.0 °C
7690 psi

@Temperature 194 °F
ISO 527
LATI LATAN 13 G/303 30% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)  (discontinued **)
Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Kleerdex Kydex® IM90 Acrylic/PVC injection Molding Compound  (discontinued **)
Low heat release aviation gradeApplications: Kydex IM90 is designed for injection molded parts each need to meet the highest flammability requirements of the FAA (FAR 25.853d) for vertical burn, rat..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Kleerdex Kydex® P55 Acrylic/PVC Extrusion Compound  (discontinued **)
Weatherable profile extrusion compoundApplications: Extruded profiles requiring weatherability, high flexural modulus, and excellent flammability resistance. Features: Weatherability is dependent o..
Tensile Strength, Ultimate 53.0 MPa
7680 psi
ASTM D412
SK Chemicals SKYTHANE® 198A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Ultimate 53.0 MPa
7680 psi
ASTM D412
SK Chemicals SKYTHANE® S198A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Plenco 00757 Melamine-Phenolic, Granular, Transfer Molded
PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Plenco 2571 Phenolic, Granular, Compression Molded
PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Plenco 3509 Phenolic, Granular, Injection Molded
PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Plenco 4414 Phenolic, Granular, Injection Molded
PLENCO 04414 is a flock and mineral filled phenolic molding compound. It is formulated for use in electrical applications that require improved heat resistance, mechanical strength, and dimensional ..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Plenco 4485 Phenolic, Granular, Compression Molded
PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Plenco 4527 Phenolic, Granular, Injection Molded
PLENCO 04527 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength, and resistance to cracking in a wet-dry environment. UL recognized under..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Plenco 6990 Phenolic, Briquette, Injection Molded
PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Plenco 7507 Phenolic, Granular, Injection Molded
PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ISO 527-1, 2
Polyplastics Duranex® 600JP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, Low melting point
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ISO 527-1, 2
Polyplastics Duranex® 6300B Polybutylene Terephthalate (PBT), Anisotropy improvement, 30% GB filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ISO 527-1, 2
Polyplastics Duranex® 800FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, Super High Viscosity
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Plenco 4300 Phenolic, Granular, Injection Molded
PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Plenco 4568 Phenolic, Granular, Compression Molded
PLENCO 04568 is a heat resistant, mineral and flock filled, phenolic molding compound, formulated to provide thermal oxidation stability along with excellent dimensional stability. 04568 is availabl..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Plenco 7523 Phenolic, Granular, Transfer Molded
PLENCO 07523 is a woodflour and cotton flock filled novolac phenolic molding compound, formulated for high impact industrial uses. UL recognized under component file E40654.Information supplied by P..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ISO 527-1, 2
Polyplastics Duranex® 700FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, High Viscosity
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Toyobo Vylopet® EMC405A PET/PBT Blend
Key Feature: HB UL-94 ClassApplications: glossy surface componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, good mechanical properties, hi..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ISO 37
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Eastman DURASTAR DS2010 Natural PCTA Copolyester
DURASTAR DS2010 polymer contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing cha..
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D651
Resinoid 1320 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D651
Resinoid 1329 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Plenco 7307 Phenolic, Granular, Transfer Molded
PLENCO 07307 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength properties. Type ASTM 5948 CFG, and UL recognized under component file E40654. 07307 is a..
Tensile Strength, Ultimate 53.0 - 76.0 MPa
7690 - 11000 psi
Average value: 61.7 MPa Grade Count:12
Overview of materials for Melamine-Phenolic Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap..
Copyright © lookpolymers.com All Rights Reserved