Plenco 7523 Phenolic, Granular, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic; Wood and Flock filled; Molded
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7523 Phenolic, Granular, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PLENCO 07523 is a woodflour and cotton flock filled novolac phenolic molding compound, formulated for high impact industrial uses. UL recognized under component file E40654.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.550 g/cc
0.0199 lb/in³
ASTM D1895
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Water Absorption 0.40 %
0.40 %
ASTM D570
Linear Mold Shrinkage 0.0079 cm/cm
0.0079 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 84
84
ASTM D785
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Elongation at Break 0.82 %
0.82 %
ASTM D638
Tensile Modulus 7.50 GPa
1090 ksi
ASTM D638
Flexural Strength 68.0 MPa
9860 psi
ASTM D790
Flexural Modulus 6.80 GPa
986 ksi
ASTM D790
Compressive Strength 194 MPa
28100 psi
ASTM D695
Izod Impact, Notched 0.192 J/cm
0.360 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.199 J/cm²
0.947 ft-lb/in²
ASTM D256
Impact 118
118
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C

@Temperature 40.0 - 130 °C
33.3 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 200 °C
392 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 158 °C
316 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Shrinkage 0.267 %
0.267 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.80e+11 ohm-cm
2.80e+11 ohm-cm
ASTM D247
Dielectric Constant 4.9
4.9
ASTM D150
Dielectric Strength 10.9 kV/mm
277 kV/in
Short Time; ASTM D149
Dissipation Factor 0.054
0.054
ASTM D150
Arc Resistance 133 sec
133 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638