Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 39.2 - 53.0 MPa | 5690 - 7690 psi | Average value: 47.9 MPa Grade Count:13 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Tensile Strength, Ultimate | 39.2 MPa | 5690 psi | ASTM D638 |
Kolon DIAMAT® EH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Tensile Strength, Ultimate | 39.2 MPa | 5690 psi | ASTM D638 |
Kolon DIAMAT® IH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Tensile Strength, Ultimate | 39.2 MPa | 5690 psi | DIN 53455; ASTM D638 |
Kolon KOPEL® KP3372 General Purpose TPE Resin KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very.. |
|||
Tensile Strength, Ultimate | 39.2 MPa | 5690 psi | |
Shinil Chemical SHINCON ABS Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Tensile Strength, Ultimate | 39.2 MPa | 5690 psi | |
Shinil Chemical SHINSTAT PCTG Electrostatic Control Polymer Sheet Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Tensile Strength, Ultimate | 39.2 MPa | 5690 psi | |
Shinil Chemical SHINSTAT PE Electrostatic Control Polymer Sheet Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Tensile Strength, Ultimate | 39.2 MPa | 5690 psi | ASTM D412 |
SK Chemicals SKYTHANE® 185A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 39.2 MPa | 5690 psi | ASTM D412 |
SK Chemicals SKYTHANE® S185A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 39.2 MPa | 5690 psi | ASTM D638 |
SK Chemicals SKYTHANE® U0251M Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 39.2 MPa | 5690 psi | ASTM D638 |
SK Chemicals SKYTHANE® UB601 Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta.. |
|||
Tensile Strength, Ultimate | 39.2 MPa | 5690 psi | ASTM D638 |
SK Chemicals SKYTHANE® US210 Magnetic Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 39.2 MPa | 5690 psi | ASTM D412 |
Lubrizol Estane® S185A Thermoplastic Polyurethane Type: Estane® S185A is a Shore 87A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Prov.. |
|||
Tensile Strength, Ultimate | 39.2 MPa | 5690 psi | |
Lubrizol Estane® UB601 Thermoplastic Polyurethane Type: Estane® UB601 resin is a linear, hydroxyl terminated polyurethane polymer designed to be used as a binder for ink formulations. For ink applications, it gives high hardness to coated surface.. |
|||
Tensile Strength, Ultimate | 39.2 MPa | 5690 psi | ASTM D412 |
Lubrizol Estane® X-595A-3FR Thermoplastic Polyurethane Type: Estane® X595A-3FR TPU is a Shore 94A, polyester type thermoplastic polyurethane elastomer.Uses: Film Blowing, Extrusion.Available in AsiaInformation Provided by The Lubrizol Corporation |
|||
Tensile Strength, Ultimate | 39.2 MPa | 5690 psi | ASTM D412 |
Lubrizol Estane® 2355-80AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Damping capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009... |
|||
Tensile Strength, Ultimate | 39.2 MPa @Temperature 260 °C |
5690 psi @Temperature 500 °F |
ASTM D1708 |
Daelim H&L Plavis-C CM Conductive Polyimide Bearing Compression Molded. Plavis-C: Conductive, Electrical conductive, high thermal resistance and superior mechanical properties. Surface resistivity 10²-10³ OhmGeneral Plavis information for all grad.. |
|||
Tensile Strength, Ultimate | 39.2 MPa @Temperature 260 °C |
5690 psi @Temperature 500 °F |
ASTM D1708 |
Daelim H&L Plavis-ESD CM Polyimide Bearing Compression Molded. Plavis-ESD: Electrostatic dissipative, Electrostatic dissipative, high thermal resistance and superior mechanical properties. And surface resistivity 10²-10³ OhmGeneral Plavis.. |
|||
Tensile Strength, Ultimate | 39.2 MPa | 5690 psi | ASTM D1708 |
Daelim H&L Plavis-N CM Unfilled Aromatic Polyimide Bearing Compression Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS po.. |
|||
Tensile Strength, Ultimate | 39.2 MPa @Temperature 260 °C |
5690 psi @Temperature 500 °F |
ASTM D1708 |
Daelim H&L Plavis-N DF Unfilled Aromatic Polyimide Bearing Direct Formed. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS polyimi.. |
|||
Tensile Strength, Ultimate | 39.2 MPa | 5690 psi | ASTM D638 |
Samyang Triel® 5700 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5700 is an extrusion grade.Information provided by Samyang. |