Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 34.0 MPa @Temperature 900 °C |
4930 psi @Temperature 1650 °F |
|
Resistalloy International Fecralloy™ 145 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kiln.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
Chevron Phillips HiD® 9308 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification: 345460A; ASTM D 4976 Classification: PE 235, A 56607Applications:Base Resin for use in Oil Patch and Industrial Pipe Appl.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
Chevron Phillips HiD® 9326 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification: 335440A; ASTM D 4976 Classification: PE 235, A 56606Applications:Base Resin for use in Oil Patch and Industrial Pipe Appl.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
Chevron Phillips HiD® 9348 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification: 335440A; ASTM D 4976 Classification: PE 235, A 56606Applications:Base Resin for use in Oil Patch and Industrial Pipe Appl.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
Chevron Phillips HiD® 9398T HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; ASTM D 3350 Classification: 345420A; ASTM D 4976 Classification: PE 235, A 56601Applications:Base Resin for use in Utility and Conduit Pipe ApplicationsData provided by.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
Chevron Phillips HiD® 9646T HDPE High Molecular Weight Sheeting Resin
(discontinued **) Resin Type: Linear Copolymer; ASTM D 4976 Classification: PE 235, A 56606Applications:Sheeting, Thermoforming, Profile ExtrusionData provided by Chevron Chemical. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
PolyOne Stat-Tech™ AS-15CP/000 ABS - 15% Carbon Powder
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
PolyOne Lubri-Tech™ ATH-000/05M Acetal Homopolymer - 5% MoS2
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 34.0 - 138 MPa | 4930 - 20000 psi | Average value: 76.3 MPa Grade Count:61 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Tensile Strength, Ultimate | 34.0 - 74.0 MPa | 4930 - 10700 psi | Average value: 54.7 MPa Grade Count:3 |
Overview of materials for Phenolic/Rubber; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | |
Kuraray HYBRAR® PH6 Polypropylene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
Sumitomo Bakelite North America FM 4005X4648 Fiberglass Reinforced Phenolic Novolac FM 4005X4648 a fiberglass reinforced phenolic novolac molding compound formulated to increase thermal conductivity and electrical conductance. This material also exhibits low post mold shrinkage.In.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | 20 in/min, at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1185 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
Plenco 1500 Polyester, Granular, Compression Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | 20 in/min, at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1185 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | 20 in/min, at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1185 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
Total PPH 3281 Polypropylene, Extrusion Grade Low melt flow homopolymer for sheet extrusion, strapping, and in-line thermoforming applicationsMelt Strength – The high melt strength of FINA 3281 allows uniform drawdown during processing, result.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
Toyobo A1080A Thermoplastic Polyurethane Elastomer, Injection Grade Polybutyleneadipate type, the most general purpose type of Toyobo Polyurethane; features excellent cost-performance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes,.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | DIN 53504 |
Lubrizol ESTANE® 5799 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | 5 mm/min |
Arkema Group Rilsan® BMN Y BZ TL Nylon 11, Bronze Bead Filled (Conditioned) Designation ISO 1874-PA11,MHLS,16-020,(Z+M)(B+D)(80BZ+05)Rigid grade with bronze beads (85%) and molybdenum fillers for injection molding. Available color: steel brown. Light and heat stabilized.No .. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D412 |
BASF Elastollan® S85A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fue.. |
|||
Tensile Strength, Ultimate | 34.0 MPa @Temperature 900 °C |
4930 psi @Temperature 1650 °F |
|
Resistalloy International Fecralloy™ 135 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire, bar, and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small .. |
|||
Tensile Strength, Ultimate | 34.0 MPa @Temperature 90.0 °C |
4930 psi @Temperature 194 °F |
ISO 527 |
LATI LARIL 13-V1 Polyphenylene Oxide (PPOm) (UL94V-1)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |