Material Notes:
Ferritic stainless steel with aluminum. Available as wire. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of atmospheres. "Fecralloy"** an Fe-Cr-Al steel containing "yttrium" is a versatile alloy and is suitable for use over a wide range up to 1300°C. The "yttrium" is the key to its longer high temperature life, having greater oxidation resistance and form stability over other resistance alloys.**"Fecralloy" is the registered trademark of the UK Atomic Energy Authority (Now AEA Technology, Harwell). Information provided by Resistalloy International Limited.
Physical Properties Metric English Comments
Density 7.10 g/cc
0.257 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 230
230
Tensile Strength, Ultimate 750 MPa
109000 psi
34.0 MPa

@Temperature 900 °C
4930 psi

@Temperature 1650 °F
Tensile Strength, Yield 550 MPa
79800 psi
Elongation at Break 16 - 20 %

@Thickness 50.0 mm
16 - 20 %

@Thickness 1.97 in
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 20.0 - 250 °C
6.11 µin/in-°F

@Temperature 68.0 - 482 °F
12.0 µm/m-°C

@Temperature 20.0 - 500 °C
6.67 µin/in-°F

@Temperature 68.0 - 932 °F
15.0 µm/m-°C

@Temperature 20.0 - 1000 °C
8.33 µin/in-°F

@Temperature 68.0 - 1830 °F
Specific Heat Capacity 0.460 J/g-°C
0.110 BTU/lb-°F
Thermal Conductivity 16.0 W/m-K
111 BTU-in/hr-ft²-°F
Melting Point 1500 °C
2730 °F
Maximum Service Temperature, Air 1400 °C
2550 °F
Optical Properties Metric English Comments
Emissivity (0-1) 0.70
0.70
Fully Oxidized
Component Elements Properties Metric English Comments
Aluminum, Al 5.8 %
5.8 %
Chromium, Cr 22 %
22 %
Iron, Fe 72 %
72 %
As remainder
Electrical Properties Metric English Comments
Electrical Resistivity 0.000145 ohm-cm
0.000145 ohm-cm
Temperature Factor is 1.03 at 800°C (1470°F). Temperature Factor is 1.04 at 1000°C (1830°F). Temperature Factor is 1.04 at 1200°C (2190°F).
Curie Temperature 600 °C
1110 °F