Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYPUR™ FPU 1185 Thermoplastic Polyurethane Compound

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded , Polyurethane, TP
Manufacturer A. Schulman, Inc.
Trade Name POLYPUR™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYPUR™ FPU 1185 Thermoplastic Polyurethane Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
15 sec delay; ASTM D2240
Tensile Strength, Ultimate 34.0 MPa
4930 psi
20 in/min, at max load; ASTM D638
Elongation at Break 500 %
500 %
ASTM D412
Flexural Modulus 0.0270 GPa
3.92 ksi
1.3 mm/min; ASTM D790
Tear Strength 87.7 kN/m
500 pli
2 in/min; ASTM D624
Compression Set 16 %
16 %
Method B, 22 h, 23°C; ASTM D395
65 %
65 %
Method B, 22 h, 70°C; ASTM D395
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved