Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 186 MPa | 27000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ PK-30CF/10T Polyetheretherketone (PEEK), Carbon Fiber Reinforced, PTFE Lubricated
(discon Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 186 MPa | 27000 psi | ASTM D638 |
Quantum Composites QC-3450 48% Glass Fiber High Temperature Use SMC
(discontinued **) QC-3450 is highly reinforced with glass fibers. It is designed for compression molding of components requiring high structural strength and good resistance to elevated temperatures. Long-term use .. |
|||
Tensile Strength, Ultimate | 186 MPa | 27000 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN133G43SIBL G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Tensile Strength, Ultimate | 186 MPa | 27000 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN333G33CR G/F Reinforced Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Tensile Strength, Ultimate | 186 MPa | 27000 psi | |
MTI ThermoStran® TPU-40G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Tensile Strength, Ultimate | 186 MPa | 27000 psi | ASTM D638 |
Lubrizol Isoplast® 101LGF40BLK Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Strength, Ultimate | 186 MPa | 27000 psi | ASTM D638 |
Lubrizol Isoplast® 101LGF40NAT Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Strength, Ultimate | 186 MPa | 27000 psi | ASTM D638 |
Lubrizol Isoplast® 202LGF40 Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Strength, Ultimate | 186 MPa | 27000 psi | |
Universal Wire Works 4043 (AMS 4190) Aluminum Alloy Filler Metal Alloy 4043 is a 5% silicon aluminum alloy designed to weld many similar and dissimilar cast and wrought aluminum parts. This alloy is excellent for types 4043, 6063, 5052, 6061, 355, 356 and others... |
|||
Tensile Strength, Ultimate | 186 MPa | 27000 psi | annealed |
CMW® D50F Silver Nickel Alloy CMW® D50F can be fabricated into wire, rod and strip; however, the headability of CMW® D50F is limited to a narrow range. It is used for main contacts in circuit breakers and switching devices whe.. |
|||
Tensile Strength, Ultimate | 186 MPa @Temperature 593 °C |
27000 psi @Temperature 1100 °F |
|
Dura-Bar 65-45-12 HRDS Continuously Cast Ductile Iron Bar Stock ASTM A536 Dura-Bar 4512 HRDS is a high-silicon ductile iron intended for use at elevated temperatures or when a part is subjected to thermal cycling, such as permanent mold applications. The ferritic structu.. |
|||
Tensile Strength, Ultimate | 186 MPa | 27000 psi | Annealed |
CMW® D54X Post-oxidized Silver Cadmium Oxide Contact Material ASTM B781, Table 3 For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc. |
|||
Tensile Strength, Ultimate | 186 MPa | 27000 psi | annealed |
CMW® ELKONIUM 45 Silver Alloy The alloying of small amounts of one of the precious metals, platinum, palladium or gold with silver increases the hardness, and reduces the metal transfer tendency. These alloys maintain a low cont.. |
|||
Tensile Strength, Ultimate | 186 MPa | 27000 psi | ASTM D638 |
Adell AR-37 Nylon 66, 35% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 186 MPa | 27000 psi | ASTM D638 |
Adell AW-17 Nylon 66, 35% Glass Reinforced; Superior Finish Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 186 MPa | 27000 psi | 5mm/min; ASTM D638 |
Asia International Enterprise (Hong Kong) 60G6 Nylon 66, 30% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Tensile Strength, Ultimate | 186 MPa | 27000 psi | ASTM D638 |
Adell AR-17 Nylon 66, 35% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 186 MPa | 27000 psi | ASTM D638 |
Adell AW-37 Nylon 66, 35% Glass Reinforced; Superior Finish Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 186 MPa | 27000 psi | 5mm/min; ASTM D638 |
Asia International Enterprise (Hong Kong) 60G7F Nylon 66, 35% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Tensile Strength, Ultimate | 186 MPa | 27000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ NI-30CF/10T-2S Nylon 6/10, Carbon Fiber Reinforced, PTFE/Silicone Lubricated
(discontinue Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |