Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.2mm and 5VB at 1... |
|||
Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Asia Pacific) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® HCX1640 PC+ABS (Europe-Africa-Middle East) CYCOLOY™ HCX1640 a PC+ABS blend specially developed for medical devices and pharmaceutical applications requiring improved mechanical performance . It combines good flow with excellent impact and l.. |
|||
Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® XCM830 PC+ABS PC/ABS with high stiffness and impact performance |
|||
Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® XCM830 PC+ABS (Asia Pacific) PC/ABS with high stiffness and impact performance |
|||
Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® 923X PC (Asia Pacific) Lexan*923x is a UV stabilized high flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low temperatur.. |
|||
Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® CFR9131 PC COPOLYMER Lexan* CFR9131 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and .. |
|||
Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® HP6NR PC (Europe-Africa-Middle East) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® HPS6 PC Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® HPS6 PC (Europe-Africa-Middle East) Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® IFX3420Z PC (Asia Pacific) Lexan* IFX3420Z is a medium viscosity, release containing, injection moldable, polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grades meets the transm.. |
|||
Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® IR2040 PC (Europe-Africa-Middle East) IR2040 resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. Food contact approved.. |
|||
Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® IR2240 PC (Europe-Africa-Middle East) IR 2240 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. Food contact approved |
|||
Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® LUX9130C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® PC1000 PC (Europe-Africa-Middle East) PC1000 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele.. |
|||
Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® PC1000R PC (Europe-Africa-Middle East) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® PC1800 PC (Asia Pacific) PC1800 resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel.. |
|||
Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® PC1800R PC (Europe-Africa-Middle East) PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® VR2220 PC (Europe-Africa-Middle East) VR2220 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® HP6NR PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® HP6NR PC (Asia Pacific) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics PC0703 PC (Europe-Africa-Middle East) PC0703 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product designed for use in the extrusion market. |
|||
Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics PC0703R PC (Asia Pacific) PC0703R resin is a low flow (MFR = 7 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the extrusion market. |
|||
Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics PC0800 PC (Asia Pacific) PC0800 resin is a low flow (MFR = 8 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics PC1000R PC (Europe-Africa-Middle East) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics PC1800 PC (Europe-Africa-Middle East) PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® ENH2900 PBT+PC (Asia Pacific) Xenoy* ENH2900 is a Non-Braominated, Non Chlorinated flame retarded PC/PBT resin with good flow, high impact and excellent chemical resistance. It was designed quite suitable for E&E housing applic.. |
|||
Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL HH180 PPE+PS (Asia Pacific) Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |