Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 9.81 - 19.6 MPa @Temperature 110 °C, Time 86400 sec |
1420 - 2840 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories CT-140 Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 9.81 - 19.6 MPa @Temperature 1000 °C, Time 10800 sec |
1420 - 2840 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories CT-140 Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 9.81 - 19.6 MPa @Temperature 1350 °C, Time 10800 sec |
1420 - 2840 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories CT-140 Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 9.81 - 19.6 MPa @Temperature 110 °C, Time 86400 sec |
1420 - 2840 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HACT-165G High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 9.81 - 19.6 MPa @Temperature 1350 °C, Time 10800 sec |
1420 - 2840 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-160 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 9.81 - 19.6 MPa @Temperature 1500 °C, Time 10800 sec |
1420 - 2840 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-170 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 9.81 - 19.6 MPa @Temperature 110 °C, Time 86400 sec |
1420 - 2840 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories INCT-170 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 9.81 - 19.6 MPa @Temperature 110 °C, Time 86400 sec |
1420 - 2840 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories MIX-1(1:4) Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 9.81 - 19.6 MPa @Temperature 110 °C, Time 86400 sec |
1420 - 2840 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories PTC-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 19.6 MPa @Temperature 110 °C, Time 86400 sec |
2130 - 2840 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories PTF-180 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 9.81 - 19.6 MPa @Temperature 110 °C, Time 86400 sec |
1420 - 2840 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories CT-130 Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 9.81 - 19.6 MPa @Temperature 110 °C, Time 86400 sec |
1420 - 2840 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories TPA-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 9.81 - 19.6 MPa @Temperature 1000 °C, Time 10800 sec |
1420 - 2840 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-160 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 19.6 MPa @Temperature 1000 °C, Time 10800 sec |
2130 - 2840 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-165 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |