Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1350 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories CT-140S Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1350 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-170 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 29.4 - 34.3 MPa @Temperature 1000 °C, Time 10800 sec |
4270 - 4980 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-180G High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1500 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1500 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1350 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PTA-180 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1350 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PTC-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1350 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PTF-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |