Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 75.0 MPa @Strain 2 % |
10900 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Ketron® 1000 PEEK unfilled, extruded (ISO Data) Ketron PEEK-1000 stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron PEEK grades. Both Ketron PEEK-1000 natural & black.. |
|||
Compressive Strength | 75.0 MPa @Temperature 200 °C |
10900 psi @Temperature 392 °F |
ISO 604 |
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp.. |
|||
Compressive Strength | 75.0 MPa @Temperature 200 °C |
10900 psi @Temperature 392 °F |
ISO 604 |
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c.. |
|||
Compressive Strength | 75.0 MPa @Temperature 200 °C |
10900 psi @Temperature 392 °F |
ISO 604 |
Victrex® WG102™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c.. |
|||
Compressive Strength | 75.0 - 85.0 MPa @Temperature 100 °C |
10900 - 12300 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 140 Dense Vibrating Refractory Castable Description: Vibron 140 is a low cement castable, based on high quality chamotte.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 75.0 - 85.0 MPa @Temperature 100 °C |
10900 - 12300 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 150 Al RAPID Dense Vibrating Refractory Castable Description: Vibron 150 Al Rapid is a vibrating low cement castable resistant to liquid aluminum metal. Due to a special additive a relatively high heating rate is possible.Remarks: These values app.. |
|||
Compressive Strength | 75.0 - 85.0 MPa @Temperature 100 °C |
10900 - 12300 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 150 Dense Vibrating Refractory Castable Description: Vibron 150 is a low cement castable based on sintered bauxite.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 75.0 - 85.0 MPa @Temperature 100 °C |
10900 - 12300 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 160 Dense Vibrating Refractory Castable Description: Vibron 160 is a low cement vibrating castable on andalusite base, characterized by a high strength and excellent thermal shock resistance.Remarks: Indicated values apply to vibrated pro.. |
|||
Compressive Strength | 75.0 - 85.0 MPa @Temperature 100 °C |
10900 - 12300 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 160 H GS (R) Dense Vibrating Refractory Castable Description: Vibron 160 H GS (R) is a pumpable low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock-, corrosion- and abrasion resista.. |
|||
Compressive Strength | 75.0 - 85.0 MPa @Temperature 100 °C |
10900 - 12300 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 170 M Dense Vibrating Refractory Castable Description: Vibron 170 is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid slags.Remar.. |
|||
Compressive Strength | 75.0 - 85.0 MPa @Temperature 100 °C |
10900 - 12300 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 170 M GS (R) Dense Vibrating Refractory Castable Description: Vibron 170 M GS (R) is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sl.. |
|||
Compressive Strength | 75.0 - 85.0 MPa @Temperature 100 °C |
10900 - 12300 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 120 S Dense Refractory Castable Description: A very strong castable with a high abrasion resistance of which both aggregate and cement attribute to hydraulic binding.Remarks: These values apply to cast products. Also available in .. |
|||
Compressive Strength | 75.0 - 85.0 MPa @Temperature 100 °C |
10900 - 12300 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 14 S Dense Refractory Castable Description: Curon 14 S is a dense, strong and abrasion resistant castable. Because of the very low percentage of Fe2O3 and SiO2 it is used for highly abrasive conditions in reducing atmospheres.Rem.. |
|||
Compressive Strength | 75.0 - 85.0 MPa @Temperature 100 °C |
10900 - 12300 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 160 H RAPID Dense Vibrating Refractory Castable Description: Vibron 160 H Rap is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance. Because of special additives, thi.. |
|||
Compressive Strength | 75.0 - 85.0 MPa @Temperature 100 °C |
10900 - 12300 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 170 M RAPID Dense Vibrating Refractory Castable Description: Vibron 170 M Rapid is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sla.. |
|||
Compressive Strength | 75.0 - 85.0 MPa @Temperature 100 °C |
10900 - 12300 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 180 Dense Vibrating Refractory Castable Description: Vibron 180 is a low cement castable with an alumina bond. The material is supplied in two components. The B component is a liquid.Remarks: Indicated values apply to vibrated products.In.. |