Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.00 GPa @Temperature 90.0 °C |
145 ksi @Temperature 194 °F |
|
LATI Latene® 7H2W TR/40 PP Homopolymer, Mineral Reinforced, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Tensile Modulus | 1.00 GPa @Temperature 90.0 °C |
145 ksi @Temperature 194 °F |
|
LATI Latene® 7H2W T-V0E PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle.. |
|||
Tensile Modulus | 1.00 GPa @Temperature 90.0 °C |
145 ksi @Temperature 194 °F |
|
LATI Kelon® B FR H CET/05-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur.. |
|||
Tensile Modulus | 1.00 GPa @Temperature 90.0 °C |
145 ksi @Temperature 194 °F |
|
LATI Latan 2 POM Polyoxymethylene (POM). Unfilled. High viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Tensile Modulus | 1.00 GPa @Temperature 60.0 °C |
145 ksi @Temperature 140 °F |
|
LATI Latene® EP 22UVH2 MX/25 PP Copolymer, Mineral Reinforced Polypropylene copolymer (PPc) based compound. UV stabilized. Improved thermal stabilization. Special mineral filler. Very good surface appearance. Good elongation.Availability: Africa & Middle East;.. |
|||
Tensile Modulus | 1.00 GPa @Temperature 70.0 °C |
145 ksi @Temperature 158 °F |
|
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Tensile Modulus | 1.00 GPa @Temperature 260 °C |
145 ksi @Temperature 500 °F |
ASTM D 638 |
Saint-Gobain Meldin® 2021 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |
|||
Tensile Modulus | 1.00 GPa @Temperature 90.0 °C |
145 ksi @Temperature 194 °F |
|
LATI Later 4-V0 PBT, Flame Retardant Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide freeAvailability: Africa & Middle East; Asia Pacific; Europe; L.. |
|||
Tensile Modulus | 1.00 GPa @Temperature 120 °C |
145 ksi @Temperature 248 °F |
|
LATI Latiblend 7587 E61-V0 PBT/PC, Flame Retardant Blend based on Polybutylene Terephthalate (PBT) / Polycarbonate (PC). Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. High impact re.. |