Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | >= 3.51 kN/m | >= 20.0 pli | steel/steel |
Resinlab® AR 4400 Metal & Composite Bonding Methacrylate Adhesive Resinlab™ AR 4400 is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in any .. |
|||
Peel Strength | 3.51 - 4.38 kN/m | 20.0 - 25.0 pli | |
ITW Devcon 10 minuteâ„¢ Epoxy, Black Information provided by ITW Devcon |
|||
Peel Strength | >= 3.51 kN/m | >= 20.0 pli | |
Master Bond EP21TDCHT-LO Room Temperature Curing, Toughened Two Component Epoxy Master Bond Polymer Adhesive EP21TDCHT-LO is a two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a very forgiving and convenient one .. |
|||
Peel Strength | >= 3.51 kN/m | >= 20.0 pli | T-peel |
Master Bond EP21TDCN Two Component Nickel Conductive Epoxy Adhesive Product Description: Master Bond Polymer System EP21TDCN is a two component, nickel filled, electrically conductive, adhesive for high performance bonding, formulated to cure at room temperature or .. |
|||
Peel Strength | >= 3.51 kN/m | >= 20.0 pli | |
Master Bond EP21TDCSFL Flexible Two Component Silver Conductive Epoxy Master Bond Polymer System EP21TDCSFL is a two component, silver filled, electrically conductive system for high performance bonding and sealing formulated to cure at room temperature or more rapidl.. |
|||
Peel Strength | >= 3.51 kN/m | >= 20.0 pli | |
Master Bond EP79FL Two Component Silver Nickel Conductive Epoxy Adhesive Master Bond Polymer System EP79FL is a two component, silver-coated nickel, electrically conductive system for high performance bonding and sealing. Its most salient features are its high flexibilit.. |
|||
Peel Strength | >= 3.51 kN/m | >= 20.0 pli | T-peel, Al to Al, 30 minute cure at 250°F |
Master Bond Supreme 3HT-80 High Strength Epoxy Adhesive Cures at 80°C Description: Master Bond Supreme 3HT-80 is a one component, heat curing epoxy system featuring excellent physical strength properties and toughness with an eye-catching curing temperature of 170-175.. |
|||
Peel Strength | >= 3.51 kN/m | >= 20.0 pli | Al/Al |
Master Bond Supreme 3HTND-1SM Fast Curing, One Component, Surface Mount Adhesive Master Bond Polymer System Supreme 3HTND-1SM is a one component, exceptionally fast curing surface mount adhesive system with exceptional toughness and durability. It has high shear and peel strengt.. |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | |
Tra-Con Tra-Bond 724-14C Polyurethane Adhesive TRA-BOND 724-14C premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong, resilient bonds to a wide variety of substrates, including aluminum, solder, nylon, mylar.. |
|||
Peel Strength | 3.51 kN/m @Temperature 82.2 °C |
20.0 pli @Temperature 180 °F |
T-Peel, 2 hrs @ 250°F, Metal Clamp Pressure, 6061 T6 FPL Etched |
Zyvex Performance Materials Aroply™ 250 Nano-Engineered Composite Film Adhesive Aroply™ 250 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported knitted nylon carrier. Cured adhe.. |
|||
Peel Strength | >= 3.51 kN/m | >= 20.0 pli | polycarbonate/polycarbonate |
Master Bond EP40 High Shear and Peel Strength, Two Component, Flexible Epoxy Master Bond Polymer System EP40 is newly developed two component highly flexible epoxy compound for high performance bonding, potting, encapsulation, and sealing with outstanding shear and peel stre.. |
|||
Peel Strength | 3.51 - 8.77 kN/m | 20.0 - 50.0 pli | Varies with substrates. |
Loctite® Durabond® E-120HP Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | |
Dow Corning 737 NEUTRAL CURE SEALANT RTV adhesive/sealant with primerless adhesion to most materialsInformation provided by Dow Corning |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | |
Dow Corning 739 PLASTIC ADHESIVE One-part, white, moisture cure RTV, non-flowing, general purpose, UL 94 HB, good adhesion.Information provided by Dow Corning |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | |
Dow Corning 786 SILICONE MILDEW RESISTANT SEALANT Dow Corning® 786 Silicone Sealant is designed to seal nonporous surfaces around showers, tubs, sinks and plumbing fixtures where conditions of high humidity and temperature extremes exist.Informati.. |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | Bond Strength; Arlon SQA-TMS-011 |
Arlon R30711R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: PolyethyleneAppearance: Red silicone gum .. |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | on canvas |
3M Scotch-Weld™ 6116 Bulk only Adhesive Same as 6111 but Lower than normal viscosity and mainly used on fabrics.Information provided by 3M |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | T-Peel |
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | T-Peel |
3M Scotch-Weld™ DP810NS Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | ABS, 180° after aging 1-2 days @ RT and 1 day |
3M Scotch-Weld™ Hi-Strength Postforming 4693 High Performance Industrial Plastic Adhesives Features:Low viscosity grade for spray or brush applicationClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstanding bond strengt.. |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | Phenolic Board, 180° after aging 1-2 days @ RT and 1 day |
3M Scotch-Weld™ Hi-Strength Postforming 4693 High Performance Industrial Plastic Adhesives Features:Low viscosity grade for spray or brush applicationClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstanding bond strengt.. |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | PVC, Hi-Impact, 180° after aging 1-2 days @ RT and 1 day |
3M Scotch-Weld™ Hi-Strength Postforming 4693 High Performance Industrial Plastic Adhesives Features:Low viscosity grade for spray or brush applicationClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstanding bond strengt.. |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | ABS, 180° after aging 1-2 days @ RT and 1 day |
3M Scotch-Weld™ Hi-Strength Postforming 4693H High Performance Industrial Plastic Adhesives Features: High Viscosity grade in collapsible tubes for flow applicationsClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstandin.. |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | Phenolic Board, 180° after aging 1-2 days @ RT and 1 day |
3M Scotch-Weld™ Hi-Strength Postforming 4693H High Performance Industrial Plastic Adhesives Features: High Viscosity grade in collapsible tubes for flow applicationsClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstandin.. |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | on canvas |
3M Scotch-Weld™ 3747 Hot Melt Adhesive General purpose for wide variety of plastics, wood and lightweight metalsInformation provided by 3M |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | T-Peel |
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Peel Strength | 3.51 kN/m @Temperature -55.0 °C |
20.0 pli @Temperature -67.0 °F |
Aluminum, Bell Peel |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |