Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 250 MPa | 36300 psi | 1.3 mm/min; ASTM D790 |
Ovation Polymers Opnyl OP66GF43 Nylon 66, As Conditioned Nylon 66-Glass reinforced(43%), high tensile strength, stiffness and HDT.Information provided by Ovation Polymers |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | ISO 178, ASTM D790 |
Nilit Nilamid A G7 FR PH1 35% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G7 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a UL 94 V0 listing 1.5 and a complete yellow card. The formulation has been optim.. |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | ISO 178, ASTM D790 |
Nilit Nilamid A3 H5 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H5 G6 has an outstanding mechanical performance and is 30% glass fiber reinforced. It is stabilized against chemical attack from peroxides and other oxidizing substances. It .. |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | ISO 178, ASTM D790 |
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i.. |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | DIN 53 452 |
Albis Plastics Tedur® L V 9107-1 PPS, 40% Glass Fiber
(discontinued **) Low Flash, Improved Impact and Burst Strength. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Pump Housings, Hollow Articles Under PressureProcessing: Injection Moldi.. |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | DIN 53 452 |
Albis Plastics Tedur® L V 9200-1 PPS, 60% Glass Fiber/Mineral
(discontinued **) Mineral-filled Grade with Improved Impact Strength, Low Mold Temp. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Shaft Seals, FlangesProcessing: Injection Molding (M.. |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4 02XT Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4 02XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve ducti.. |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | |
Idemitsu Kosan Xarec® N WA 7030 SPS, 30% Glass Filled Crystalline Polymer Blend, Glass Filled, Impact Modified |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UFL36AS is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features include Internally Lubricated, Heat Stabilized. |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp UFL36ASP PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UFL36ASP is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE.
Added features include Internally Lubricated, Heat Stabilized.This data was supplied by SABIC-IP f.. |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp EF008EXP PEI (Europe-Africa-Middle East) LNP* Thermocomp* EF008EXP is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SABIC-IP .. |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF007H PA 66 LNP* Thermocomp* RF007H is a compound based on Nylon 66 containing glass fiber. Added feature includes: Healthcare. |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF007SXP PA 66 LNP* THERMOCOMP* RF007SXP is a compound based on Nylon 66 containing 35% Glass Fiber. Added feature of this material includes: Heat Stabilized. |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | ASTM D790 |
Techmer ES HiFill® PPS F GF/M55 BK 55% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 55% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | ASTM D790 |
Techmer ES HiFill® PPS GF/M55 BK 55% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 55% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | ASTM D790 |
Cheng Yu Plastic N6G15 Nylon 6, 15% Glass Filled |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | ASTM D790 |
Chevron Phillips Xtel® XK2340 Polyphenylene Sulfide Alloy Black Polyphenylene Sulfide AlloyXtel™ XK2340 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of toughness and.. |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | DIN 53 452 |
Albis Plastics Tedur® L 9511 PPS, 45% Glass Fiber High Strength, High Rigidity Standard Grade. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Fixture Elements, HousingsProcessing: Injection Molding (Melt Temperature:.. |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | ASTM D790 |
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® BR111 is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical .. |
|||
Flexural Yield Strength | 250 MPa | 36300 psi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4-200NA is an advanced 40% fiberglass reinforced polyphenylene sulfide compound developed to provide high strength, fast cycles, and low mainten.. |