Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 124.1 MPa | 18000 psi | ASTM D790 |
PTS Trimid® N66-100HL Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 124.1 MPa | 18000 psi | ASTM D790 |
PTS Trimid® N66-100NL Nucleated, Lubricated Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 124 - 214 MPa | 18000 - 31000 psi | Average value: 181 MPa Grade Count:17 |
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 10% Glass Fiber". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Flexural Yield Strength | 124 - 300 MPa | 18000 - 43500 psi | Average value: 197 MPa Grade Count:47 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Flexural Yield Strength | 124 - 179 MPa | 18000 - 26000 psi | Average value: 145 MPa Grade Count:3 |
Overview of materials for Nylon 11 with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ.. |
|||
Flexural Yield Strength | 124 MPa | 18000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP UX06002 PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UX06002 is a compound based on Polyphthalamide resin containing Aramide Fiber, PTFE. Added features include: Easy Molding, Internally Lubricated, Heat Stabilized. |
|||
Flexural Yield Strength | 124 MPa | 18000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Europe-Africa-Middle East) LNP* LUBRICOMP* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. Added features include: Flame Retardant, Internally Lubricated. |
|||
Flexural Yield Strength | 124 MPa | 18000 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM D9065 PEI Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Flexural Yield Strength | 124 MPa | 18000 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM D9065 PEI (Asia Pacific) Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Flexural Yield Strength | 124 MPa | 18000 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® 701 PBT (Asia Pacific) 35% glass/mineral alloy, excellent electrical performance to dielectric breakdown. Developed for automotive distributor caps.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 124 MPa | 18000 psi | ASTM D790 |
Techmer ES Luriblend® HTN 01420 BK Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: Good Wear Resistance, Low Friction, High Heat Resistance and LubricatedAppearance: BlackInformation provide.. |
|||
Flexural Yield Strength | 124 MPa | 18000 psi | ASTM D790 |
Techmer ES Plastiblend® PA6/6 HS L N Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and Nucleating AgentFeatures: Heat Stabilized, Impact Modified and NucleatedProcessing Method: Injection MoldingIn.. |
|||
Flexural Yield Strength | 124 MPa | 18000 psi | ASTM D790 |
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I.. |
|||
Flexural Yield Strength | 124 MPa | 18000 psi | ASTM D790 |
Sumitomo Bakelite Durez® 23570 Phenolic, Compression Grade Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft.. |
|||
Flexural Yield Strength | 124 MPa | 18000 psi | ASTM D790 |
Clariant PA213M40BK Nylon 6, 40% Mineral Reinforced, Heat Stabilized, Black Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 124 MPa | 18000 psi | ASTM D790 |
Clariant Renol PA101F/ST801 Nylon 66, Impact Modified, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 124 MPa | 18000 psi | ASTM D790 |
Chem Polymer Chemlon 218 GV Nylon 6, 18% Glass Reinforced A flame retardant, glass reinforced grade of nylon 6. The material is UL94 V0 rated, completely non-halogenated and phosphorus free. It gives excellent surface appearance and is available in a ran.. |
|||
Flexural Yield Strength | 124 MPa | 18000 psi | ASTM D790 |
Chem Polymer Durlex 715 G PBT, 15% Glass Reinforced A lubricated, 15% glass reinforced PBT offering a balance of rigidity, dimensional stability and toughness.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Yield Strength | 124 MPa | 18000 psi | ASTM D790 |
Chem Polymer Chemlon 104-13 G Nylon 66, 13% Glass Fiber Reinforced A toughened, 13% glass fiber reinforced nylon 66 exhibiting improved toughness and ductility, especially dry as molded.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Yield Strength | 124 MPa | 18000 psi | ASTM D790 |
Custom Resins Norpex® GF2 PPE (Polyphenylene Ether), 20% Glass Filled
(discontinued **) Properties for dry as molded samples.Data provided by the manufacturer |
|||
Flexural Yield Strength | 124 MPa | 18000 psi | ASTM D790 |
Techmer ES HiFill® TPX-HTN-01043 A Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: High Temperature Strength, Impact Modified and LubricatedUL File Number: E157318Information provided by TP C.. |
|||
Flexural Yield Strength | 124 - 165 MPa | 18000 - 24000 psi | ASTM D790 |
Premix Premi-Glas® 1200H-24 Polyester SMC
(discontinued **) Premi-Glas® 1200H-24 is a 24% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where arc resistance and dielectric strength are required and UL 94 HB flame recogni.. |
|||
Flexural Yield Strength | 124 MPa | 18000 psi | ASTM D790 |
Techmer ES HiFill FR® PBT GF15 FR X 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, In.. |