Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 86.2 MPa @Thickness 3.17 mm |
12500 psi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10FR-(VIK) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Impact Modifier and Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 86.2 MPa @Thickness 3.17 mm |
12500 psi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10R-(IM) 10 MFI Impact Modified Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 86.2 MPa @Thickness 3.17 mm |
12500 psi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10FRN (V) 15 MFI, 5VA, Flame Retardant, UV Stabilized Polycarbonate With Release ROHS Compliant.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 86.2 - 241 MPa | 12500 - 35000 psi | Average value: 181 MPa Grade Count:17 |
Overview of materials for Polyphenylene Sulfide (PPS), Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Conductive". Each property range of values reported is minimum and maximum .. |
|||
Flexural Yield Strength | 86.2 - 103 MPa | 12500 - 15000 psi | Average value: 91.6 MPa Grade Count:11 |
Overview of materials for Nylon 612, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Yield Strength | 86.2 MPa | 12500 psi | ASTM D790 |
Star Plastics PC/PET7901 Molding Grade PC/PET Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 86.2 MPa | 12500 psi | ASTM D790 |
Star Plastics PC1510FR Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 86.2 MPa | 12500 psi | ASTM D790 |
Star Plastics PC1510R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 86.2 MPa | 12500 psi | ASTM D790 |
Star Plastics PC1510R Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 86.2 MPa | 12500 psi | ASTM D790 |
Star Plastics PC1510RUV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 86.2 MPa | 12500 psi | ASTM D790 |
Star Plastics PC1510UV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 86.2 MPa | 12500 psi | ASTM D790 |
Techmer ES Plastiblend® PC/ABS 1110 Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 86.2 MPa | 12500 psi | ASTM D790 |
Techmer ES Plastiblend® PC/ABS 2022 Availability: North AmericaForms: PelletsFeatures: Low GlossInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 86.2 MPa | 12500 psi | ASTM D790 |
Techmer ES Plastiblend® PC/ABS 8001A Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 86.2 MPa | 12500 psi | ASTM D790 |
Techmer ES Statiblend® PC FR BK Availability: North AmericaForms: PelletsAntistaticFeatures: Flame Retardant and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 86.2 MPa | 12500 psi | ASTM D790 |
Star Plastics PC1212R Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 86.2 MPa | 12500 psi | ASTM D790 |
Clariant Renol PBT1100TF10 Polybutylene Terephthalate, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 86.2 MPa | 12500 psi | ASTM D790 |
Ensinger Tecaform™ HPV 13 Acetal Homopolymer - Extruded Products (POM) Tecaform™ HPV 13 is a brown homopolymer acetal with an internal PTFE lubricant. Its low coefficient of friction, excellent PV values, toughness, wear resistance, and machinability make it an excep.. |
|||
Flexural Yield Strength | 86.2 - 132 MPa | 12500 - 19100 psi | Average value: 105 MPa Grade Count:7 |
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum.. |