Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 71.0 MPa | 10300 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion LR610 white 1046 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | ASTM D790 |
Nylene® Norpex® AX245 PPE (Polyphenylene Ether) Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® FR15 ABS Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Europe-Africa-Middle East) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® EXCY0025 PC+ABS Recyle Material with PC+ABS+EXL recycle for good low temperature impact performance. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 123X PC Copolymer Improved flow PC with excellent processability and mold release. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Europe-Africa-Middle East) Improved flow PC with excellent processability and mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP AFP26 ABS (Europe-Africa-Middle East) LNP* Lubricomp* AFP26 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, PTFE, Silicone. |
|||
Flexural Yield Strength | 71.0 - 115 MPa | 10300 - 16700 psi | Average value: 97.9 MPa Grade Count:10 |
Overview of materials for Acrylic, High Flow, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app.. |
|||
Flexural Yield Strength | 71.0 - 255 MPa | 10300 - 37000 psi | Average value: 130 MPa Grade Count:176 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 50 mm/min; ASTM D790 |
LG Chemical LI-943 ASA Resin
(discontinued **) Heat resistance, Excellent weather resistance, Well balanced mechanical properties, Superior chemical resistance, Good thermal aging stability, Good moldability and processability, Applications incl.. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WL003 is a compound based on Polybutylene Terephalate resin containing PTFE. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | ASTM D790 |
Spartech Acrylloy 10 Acrylic Sheet Description: Acrylic SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | ASTM D790 |
Spartech Crylex High Impact Acrylic Sign Grade Sheet Description: Sign Grade SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | ASTM D790 |
Spartech SolarKote® /ABS Weatherable Sheet Description: Weatherable SheetSolarKote is a registered trademark of Atofina Chemicals, Inc..Information provided by Spartech. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Asia Pacific) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Asia Pacific) PC+Polyester, UV Stabilized, Transparent |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Europe-Africa-Middle East) Transparent, US Food Contact compliant, chemically resistant.
This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b.. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® K3501 PBT Unfilled PBT, Hydrollytically Stable, Heat Stabilized, Impact Modified. A hydrollytically stable grade designed for improved performance under heat/humidity environments. Targeted at automotive unde.. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester, UV Stabilized, Transparent |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | ASTM D790 |
Techmer ES HiFill® TPX-PBT-98010 BN069 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityAppearance: Light BeigeProcessing Method: Injection MoldingInformation provided by TP C.. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Asia Pacific) Improved flow PC with excellent processability and mold release. |
|||
Flexural Yield Strength | 71.0 MPa | 10300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |