| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Rigid Extrusion LR610 white 1046 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 80 <br>@Temperature 23.0 °C |
80 <br>@Temperature 73.4 °F |
ASTM D2240 |
| Tensile Strength, Yield | 39.4 MPa | 5710 psi | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 3.33 GPa | 483 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Yield Strength | 71.0 MPa | 10300 psi | ASTM D790 |
| Flexural Modulus | 2.81 GPa | 408 ksi | ASTM D790 |
| Dart Drop Total Energy | 38.7 J/cm | 0.0725 ft-lb/mil | Procedure A; ASTM D4226 |
| 38.7 J/cm | 0.0725 ft-lb/mil | Procedure B; ASTM D4226 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 61.0 µm/m-°C | 33.9 µin/in-°F | ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 78.4 °C | 173 °F | Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 74.3 °C | 166 °F | Unannealed; ASTM D648 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | General Purpose | |
| Forms | Cube | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Recycled Content | Yes | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Building Materials | |