Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 70.3 MPa | 10200 psi | ASTM D790 |
Ravago Manufacturing Americas Hylac® GP55 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Yield Strength | 70.3 MPa | 10200 psi | ASTM D790 |
PTS Trilac® ABS-HH2000 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 70.3 MPa | 10200 psi | ASTM D790 |
PTS Trilac® ABS-HS5500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 70.3 MPa | 10200 psi | ASTM D790 |
Ravago Manufacturing Americas Hysun™ 678 ASA Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families. Availibility: North America F.. |
|||
Flexural Yield Strength | 70.3 - 230 MPa | 10200 - 33400 psi | Average value: 158 MPa Grade Count:95 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Flexural Yield Strength | 70.3 MPa | 10200 psi | ASTM D790 |
PTS Trilac® ABS-HF5500 High Flow ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 70.3 MPa @Thickness 3.20 mm |
10200 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUCEL FW700N Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0Information provided by LG Chemical |
|||
Flexural Yield Strength | 70.3 MPa | 10200 psi | ASTM D570 |
LG Chemical Lupox® PBT-GP-2306FA 30% GFR Flame Retardant, UV Stabilized PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 70.3 MPa | 10200 psi | ASTM-D790 |
Ineos ABS Lustran® Guardian™ 620 ABS, Extrusion Grade Lustran® Guardian™ ABS 620 is a high modulus, HFC 134a and HCFC 22 resistant extrusion grade resin designed for refrigerator door and food liners. Lustran® ABS 620 offers good melt streng.. |
|||
Flexural Yield Strength | 70.3 MPa | 10200 psi | ASTM D790 |
TPI Porene® KU900 Super High Heat ABS INJECTION MOLDING. ELECTRICAL PARTS, AUTOMOTIVE APPLICATIONS, HOUSEHOLD GOODS, TOYSPorene® is a registered trademark of Thai Petrochemical Industry Co. LTD. Information provided by Dayson Polymer.. |
|||
Flexural Yield Strength | 70.3 MPa @Thickness 3.17 mm |
10200 psi @Thickness 0.125 in |
|
TPI Porene® ABS-GA800 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 70.3 MPa @Thickness 3.17 mm |
10200 psi @Thickness 0.125 in |
|
TPI Porene® ABS-GA850 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 70.3 MPa | 10200 psi | ASTM D790 |
PlastxWorld Veroplas PA2002 Nylon 6 general purpose, unfilled, impact modified injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 70.3 MPa | 10200 psi | ASTM D790 |
Kleerdex Kydex® 115 Acrylic/PVC Thermoplastic Sheet