Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 63.0 MPa | 9140 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® EXABS01 ABS Sheet extrusion ABS with medium impact. |
|||
Flexural Yield Strength | 63.0 MPa | 9140 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® FR15U ABS Flame retardant ABS with excellent indoor UV properties and excellent processing. UL94 V-0/5VA rated. Elevated UL RTI rating (90-85-90) for all colors except for blue and green colors (60-60-60). |
|||
Flexural Yield Strength | 63.0 MPa | 9140 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific) Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing. |
|||
Flexural Yield Strength | 63.0 MPa | 9140 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® FR15U ABS (Europe-Africa-Middle East) CYCOLAC FR15U is a flame retardant ABS with good processability and good indoor UV properties. |
|||
Flexural Yield Strength | 63.0 MPa | 9140 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® G320 ABS (Europe-Africa-Middle East) CYCOLAC G320 is a super high impact resistant ABS grade. It combines impact resistance with high stiffness, good temperature resistance and processability. It has a good fit in automotive interiors .. |
|||
Flexural Yield Strength | 63.0 MPa | 9140 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP COLORCOMP WX96084 PBT (Europe-Africa-Middle East) LNP* COLORCOMP* WX96084 is a compound based on Polybutylene Terephalate resin. Added features include: Custom Color White. |
|||
Flexural Yield Strength | 63.0 MPa | 9140 psi | ASTM D790 |
Kleerdex Vinyloy™ 100 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Utility gradeApplications: Vinyloy 100 sheet is a fire retardant that can be used to substitute effectively for ABS and other utility grade thermoplastics.Features: Vinyloy 100 sheet is a recycled g.. |
|||
Flexural Yield Strength | 63.0 MPa | 9140 psi | ASTM D790 |
Kleerdex Vinyloy™ 102 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Recycled capped FR sheetApplications: Vinyloy 102 sheet is capped sheet that can be used to substitute effectively for ABS and other grades of thermoplastic sheet for your thermoforming needs.Featur.. |
|||
Flexural Yield Strength | 63.0 - 100 MPa | 9140 - 14500 psi | Average value: 82.9 MPa Grade Count:21 |
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum .. |
|||
Flexural Yield Strength | 63.0 - 145 MPa | 9140 - 21000 psi | Average value: 107 MPa Grade Count:22 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Flexural Yield Strength | 63.0 MPa | 9140 psi | ASTM D790 |
KYDEX® V Acrylic/PC Thermoplastic Sheet Utility sheetApplications: Can be used to substitute effectively for utility grade thermoplastics. It is very appropriate for hidden parts and painted parts and/or where fire retardancy is not requ.. |
|||
Flexural Yield Strength | 63.0 MPa | 9140 psi | ASTM D790 |
Hannam Chemical Hanalac 710 ABS |
|||
Flexural Yield Strength | 63.0 MPa | 9140 psi | ASTM D790 |
Hannam Chemical Hanalac 775 ABS, Extrusion Grade Increased chemical resistance. Excellent mechanical strength, high rigidity, and high impact strength. Good thermoformability. Applications: Refrigerators liners, bathtubs, automobile interiors,.. |
|||
Flexural Yield Strength | 63.0 MPa | 9140 psi | ASTM D790 |
KYDEX® 6200 Thermoplastic Sheet Fire rated sheet for mass transitApplications: Dashboards, seatbacks, armrests, tray tables, window reveals, cabin linersFeatures: Kydex 6200 is a proprietary, high performance thermoplastic sheet. .. |
|||
Flexural Yield Strength | 63.0 MPa | 9140 psi | ASTM D790 |
Spartech Royalite R61M Low Smoke Resin Data provided by the manufacturer. Formulated to meet smoke and fire specifications recommended by the FTA, this is ideally suited for mass transit applications such as seat backs, overhead storage.. |
|||
Flexural Yield Strength | 63.0 MPa | 9140 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® 6620U PBT+PC PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance. |
|||
Flexural Yield Strength | 63.0 MPa | 9140 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON WS002I PBT LNP* STAT-KON* WS002I is a compound based on PBT resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, High Impact. |
|||
Flexural Yield Strength | 63.0 MPa | 9140 psi | ISO 178 |
Eastman Eastar MN004 Copolyester Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl.. |
|||
Flexural Yield Strength | 63.0 MPa | 9140 psi | ASTM D790 |
Chem Polymer Chemlon 109 Nylon 66, High Impact A highly impact-modified, lubricated nylon 66 exhibiting excellent toughness, especially at lower temperatures.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Yield Strength | 63.0 MPa | 9140 psi | ASTM D790 |
Kleerdex Kydex® 200 Acrylic/PVC Thermoplastic Sheet
(discontinued **) General purpose gradeApplications: Can be used to substitute effectively for both general purpose ABS and acrylic/PVC thermoplastics. Examples include data processing equipment housings, photocopy .. |