Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1000FV PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1000FV PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1000FV PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 1000RV PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 1000RV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1100FV PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1100FV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1100FV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 1100V PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 1100V PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1100V PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle Eas.. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP WFL34 PBT LNP LUBRICOMP* WFL34 is a compound based on PBT resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1000 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1000E PEI Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1000E PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem HU1000E PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1100 PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1100 PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1100 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC LNP* Thermocomp* DF004RXP is a compound based on Polycarbonate resin containing 20% Glass Fiber. Some light color grades may have lower impact data than natural and black. Added features include: .. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC (Asia Pacific) 20% Glass Fiber Reinforced Polycarbonate. Some light color grades may have lower impact data than nature and black grade. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP WCL36 PBT LNP* LUBRICOMP* WCL36 is a compound based on PBT resin containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant. |
|||
Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF PX95726 PA 6 LNP THERMOTUF* PX95726 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |