| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
| 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 | |
| Moisture Absorption | 0.0300 % | 0.0300 % | 50% RH, 24 hrs; ASTM D570 |
| 0.0500 % | 0.0500 % | 23°C / 50% RH; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm <br>@Time 86400 sec |
0.0020 - 0.0040 in/in <br>@Time 24.0 hour |
ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.010 - 0.030 cm/cm <br>@Time 86400 sec |
0.010 - 0.030 in/in <br>@Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 121 MPa | 17500 psi | 5 mm/min; ISO 527 |
| 125 MPa | 18100 psi | Type I, 5 mm/min; ASTM D638 | |
| Tensile Strength, Yield | 125 MPa | 18100 psi | Type I, 5 mm/min; ASTM D638 |
| 130 MPa | 18900 psi | 5 mm/min; ISO 527 | |
| Elongation at Break | 1.0 % | 1.0 % | Type I, 5 mm/min; ASTM D638 |
| 1.0 % | 1.0 % | 5 mm/min; ISO 527 | |
| Elongation at Yield | 1.0 % | 1.0 % | Type I, 5 mm/min; ASTM D638 |
| 1.0 % | 1.0 % | 5 mm/min; ISO 527 | |
| Tensile Modulus | 20.64 GPa | 2994 ksi | 1 mm/min; ISO 527 |
| 23.38 GPa | 3391 ksi | 50 mm/min; ASTM D638 | |
| Flexural Strength | 175 MPa | 25400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 187 MPa | 27100 psi | ISO 178 | |
| Flexural Yield Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Flexural Modulus | 14.9 GPa | 2160 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 18.06 GPa | 2619 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 0.360 J/cm | 0.674 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 3.90 J/cm | 7.31 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 6.00 J <br>@Temperature 23.0 °C |
4.43 ft-lb <br>@Temperature 73.4 °F |
ASTM D3763 |
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
| Coefficient of Friction, Dynamic | 0.34 | 0.34 | ASTM D3702 Modified |
| Coefficient of Friction, Static | 0.30 | 0.30 | ASTM D3702 Modified |
| K (wear) Factor | 4.03 - 6.04 x 10<sup>-8</sup> mm³/N-M | 2.00 - 3.00 x 10<sup>-10</sup> in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
| 50.4 x 10<sup>-8</sup> mm³/N-M | 25.0 x 10<sup>-10</sup> in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 13.0 µm/m-°C <br>@Temperature -30.0 - 30.0 °C |
7.22 µin/in-°F <br>@Temperature -22.0 - 86.0 °F |
ASTM D696 |
| CTE, linear, Transverse to Flow | 36.0 µm/m-°C <br>@Temperature -30.0 - 30.0 °C |
20.0 µin/in-°F <br>@Temperature -22.0 - 86.0 °F |
ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 223 °C | 433 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 222 °C <br>@Thickness 3.20 mm |
432 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 210 °C <br>@Thickness 3.20 mm |
410 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 |