Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CX2142ME PC+ABS Cycoloy* resin grade CX2142ME is an injection moldable PC/ABS blend with Br- and Cl-free flame retardant systems. Key features of good flow, good impact, UL-94 V0 rating at 1.2 mm, and improved chem.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX2142ME PC+ABS (Asia Pacific) Cycoloy* resin grade CX2142ME is an injection moldable PC/ABS blend with Br- and Cl-free flame retardant systems. Key features of good flow, good impact, UL-94 V0 rating at 1.2 mm, and improved chem.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CY5220 PC+ABS (Asia Pacific) Non-chlorinated & non-brominated FR PC/ABS featuring good flow and impact properties. Designed for various thin wall applicationsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS (Asia Pacific) High heat PC/ABS blend offering high modulus / low CTE and good practical impact |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® ML6430 PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML7672 PC (Asia Pacific) Non FR PC + GF, UV-Stabilizer, balanced flow & impact. Available in Opaque only. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX2471T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Europe-Africa-Middle East) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo.. |
|||
Flexural Yield Strength | >= 100 MPa | >= 14500 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® EFX830ME PC (Asia Pacific) Modified PC blend offering metallic look with minimal flow lines, flame retarded without using Chlorinated or Brominated additives.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Asia Pacific) Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Europe-Africa-Middle East) 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 100 - 433.06 MPa @Temperature -40.0 - 121 °C |
14500 - 62810 psi @Temperature -40.0 - 250 °F |
Average value: 243 MPa Grade Count:3 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA High flow PPO+PA. Power distribution box applications. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX986 PPE+PA66 (Europe-Africa-Middle East) Conductive GTX, CTE 6 |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl GTX VP7133 PPE+PA (Europe-Africa-Middle East) Noryl GTX VP7133 is an unfilled extrusion grade which offers high heat resistance in combination with high meltstrength.The material is especially designed for thermal break profiles which are used .. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Europe-Africa-Middle East) Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL EXNL1117 PPE+HIPS high gloss Noryl |
|||
Flexural Yield Strength | 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Europe-Africa-Middle East) NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |