Polymer Property : Film Tensile Strength at Break, TD = 27.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 27.6 MPa
4000 psi
ASTM D882
M. Holland Company LL104 LLDPE  (discontinued **)
Additives: Antiblock, SlipFeatures: Unspecified Antiblocking, Butene Comonomer, Copolymer, Good Drawdown, Good Processability, Unspecified SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c) 2.2..
Film Tensile Strength at Break, TD 27.6 MPa
4000 psi
ASTM D882
M. Holland Company MAGMA® LM115-B LLDPE  (discontinued **)
Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland.
Film Tensile Strength at Break, TD 27.6 - 37.9 MPa
4000 - 5500 psi
ASTM D882
Honeywell ACLAR® 22C (10.0 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe..
Film Tensile Strength at Break, TD 27.6 - 41.4 MPa
4000 - 6000 psi
ASTM D882
Honeywell ACLAR® 22C (7.50 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe..
Film Tensile Strength at Break, TD 27.6 - 41.4 MPa
4000 - 6000 psi
ASTM D882
Honeywell ACLAR® 22C (5.00 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe..
Film Tensile Strength at Break, TD 27.6 - 48.3 MPa
4000 - 7000 psi
ASTM D882
Honeywell ACLAR® UltRx 3000 CTFE Homopolymer, Barrier Film
Description: ACLAR® UltRx 3000 is a 3 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme..
Film Tensile Strength at Break, TD 27.6 MPa
4000 psi
ASTM D882
Westlake Elevate™ EF446 6.0% Ethylene Vinyl Acetate Copolymer
Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, sectio..
Film Tensile Strength at Break, TD 27.6 MPa
4000 psi
ASTM D882
Westlake Hifor Clear SC74558 Linear Low Density Polyethylene
WESTLAKE Hifor Clear Polyethylene SC74558 is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains medium slip and low antiblock additives...
Film Tensile Strength at Break, TD 27.6 MPa
4000 psi
ASTM D882
Westlake Hifor SC74557 Linear Low Density Polyethylene
WESTLAKE Hifor Clear Polyethylene SC74557 is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and low antiblock. Films produc..
Film Tensile Strength at Break, TD 27.6 MPa
4000 psi
ASTM D882
ExxonMobil LDPE LD 319.92 Low Density Polyethylene Resin
Product Description: LD 319.92 resin is an 8.7% vinyl acetate copolymer film resin. Film made from LD 319.92 exhibits superior impact strength and heat sealability.Availability: Latin America, North..
Film Tensile Strength at Break, TD 27.6 MPa
4000 psi
ASTM D882
Dow INTEGRAL™ 936 High Heat Monolayer Adhesive Film
INTEGRAL 936 High Heat Monolayer Adhesive Film is a heat-activated, thermally stable adhesive film for automotive applications capable of bonding to urethane foam-baked fabrics, paper, cardboard, fi..
Film Tensile Strength at Break, TD 27.6 MPa
4000 psi
ASTM D882
ExxonMobil Escorene® LD 720.01 Specialty Film Resin
Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou..
Film Tensile Strength at Break, TD 27.6 MPa
4000 psi
ASTM D882
ExxonMobil Escorene® LD 720.62 Specialty Film Resin
Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou..
Film Tensile Strength at Break, TD 27.6 MPa
4000 psi
3M 901 Repulpable Forms-Splicing Tape
3M™ Repulpable Forms-Splicing Tape 901 is a semi-bleached kraft paper coated with a light green repulpable adhesive.Information provided by 3M
Film Tensile Strength at Break, TD 27.6 MPa
4000 psi
3M 9114 Butt Splicing Tape
3M™ Butt Splicing Tape 9114 is a single-coated blue repulpable splicing tape which is covered with a center slit repulpable paper liner, and additionally laminated with a single coated non-repulpab..