Westlake Elevate™ EF446 6.0% Ethylene Vinyl Acetate Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Westlake Chemical Corporation
Trade Name Elevate™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Elevate™ EF446 6.0% Ethylene Vinyl Acetate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, section 177.1350. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Vinyl Acetate Content 6.0 %
6.0 %
Thickness 31.8 microns
1.25 mil
Melt Flow 2.0 g/10 min
2.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 450 %
450 %
ASTM D882
Film Elongation at Break, TD 770 %
770 %
ASTM D882
Dart Drop 7.48 g/micron
190 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
Film Tensile Strength at Break, TD 27.6 MPa
4000 psi
ASTM D882
1% Secant Modulus, MD 131 MPa
19000 psi
ASTM D882
1% Secant Modulus, TD 110 MPa
16000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 5.0 %
5.0 %
ASTM D1003
Gloss 65 %
65 %
at 45º; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 182 - 199 °C
360 - 390 °F
with BUR of 1.5:1 or higher
Blow-up Ratio (BUR) 2.5
2.5
Descriptive Properties Value Comments