Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 100 g | 0.221 lb | F50; ISO 7765-1 |
Polimeri Europa Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene Flexirene FF 25 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FF 25 is characterized by a high elongational viscosi.. |
|||
Dart Drop Test | >= 100 g | >= 0.221 lb | ASTM D1709 |
NIZHNEKAMSKNEFTEKHIM PE 5118Q (18603) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ISO 7765-1 |
Polimeri Europa Flexirene® CL 10 Butene Copolymer Linear Low Density Polyethylene Flexirene CL 10 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties.Main Applications: Flexire.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Formosa Plastics Formolene® L62608PE Film (Hexene Grade) LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he.. |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-303 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact .. |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-314 EVA Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer resin for higher clarity films. Film made from LD-314 offers good impact strength, heat sealability, and low tempera.. |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-315 EVA Packaging Film Resin for Frozen Food
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer clarity film resin. This resin's low melt index and its comonomer contact combine to provide film of special toughne.. |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-325 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Iran Petrochemical (PCC) 09X02 Linear Low Density Polyethylene 09X02 is a high performance LLDPE (HP-LLDPE) cast film grade combines ease of processing with low gels and good film strength. Its excellent stretchability makes this grade particularly suited for s.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Iran Petrochemical (PCC) LF0200 Low Density Polyethylene LF0200 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. LF0200 contains antioxidant.Applications: genera.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ISO 7765-1 |
Borealis Borstar® FB3450 HDPE for Film Extrusion Borstar® FB3450 is a high density polyethylene. Borstar® FB3450 is well suited for multilayer coextruded films where higher stiffness and toughness than in standard LDPE and LLDPE is required. Ap.. |
|||
Dart Drop Test | 100 g @Thickness 0.0400 mm |
0.221 lb @Thickness 0.00157 in |
ISO 7765-1 |
Borealis FA6220 Low Density Polyethylene FA6220 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant. This grade is developed for the production of thin blown films. Applications: shrink film, pouches, general packagin.. |
|||
Dart Drop Test | 100 g @Thickness 0.0400 mm |
0.221 lb @Thickness 0.00157 in |
ISO 7765-1 |
Borealis FA6224 Low Density Polyethylene FA6224 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed for the production of thin blown f.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Westlake EF796 Low Density Polyethylene Westlake Polyethylene EF796 is a low density formulation suggested for film applications requiring a good balance of properties such as converter film for industrial packaging and general-purpose pa.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ISO 7765-1 |
Total Lumicene® mPE M5510 EP Metallocene Polyethylene, Blown Film This product is a Total Ecosolutions grade.Lumicene® mPE M5510 EP is a second generation metallocene high density homopolymer polyethylene.Lumicene® mPE M5510 EP can be processed at high output ra.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Formosa Plastics Formolene® L62608 Film (Hexene Grade) LLDPE Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709A |
ExxonMobil LDPE LD 105.BR Low Density Polyethylene Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709A |
ExxonMobil LLDPE LL 1001X26 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709A |
ExxonMobil LLDPE LL 1001X31 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709A |
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Dart Drop Test | <= 100 g | <= 0.221 lb | Method B |
Dow TUFLIN™ HS-7046 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Slot Cast Extrusion Outstanding Drawdown Capability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7046 NT 7 is an ethylene-hexene copolymer, designed f.. |
|||
Dart Drop Test | <= 100 g | <= 0.221 lb | Method B; ASTM D1709 |
Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7066 NT 7 is a fractional melt, ethylene-hexene copolymer, designed for good toughness and stiffness. Th.. |
|||
Dart Drop Test | <= 100 g | <= 0.221 lb | Method B; ASTM D1709 |
Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7066 NT 7 is a fractional melt, ethylene-hexene copolymer, designed for good toughness and stiffness. Th.. |
|||
Dart Drop Test | <= 100 g | <= 0.221 lb | Method B; ASTM D1709 |
Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7094 NT 7 is a fractional melt, ethylene-hexene copolymer, designe.. |
|||
Dart Drop Test | <= 100 g | <= 0.221 lb | Method B; ASTM D1709 |
Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7094 NT 7 is a fractional melt, ethylene-hexene copolymer, designe.. |
|||
Dart Drop Test | 100 g | 0.221 lb | gF/50%f; ASTM D1709 |
Braskem LHB118/21AF Blown Film Extrusion Linear Low Density Polyethylene Frozen chicken packages; Meat-based frozen packages.Additives: Antiblock, D, PPA, PEBDInformation provided by Braskem. |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ASTM D1709 |
Braskem LL 218 LLDPE Cast Film Extrusion Polyethylene Description: LL218 is a Linear Low Density Polyethylene, copolymer of butene-1, produced by Spherilene process. Developed for cast film extrusion. Films obtained with this product show a good proces.. |
|||
Dart Drop Test | 100 g | 0.221 lb | g/F50; ASTM D1709 |
Braskem LL218 Cast Film Extrusion Linear Low Density Polyethylene Stretch films; Liners; LDPE and HDPE blends; Packages for general use.Information provided by Braskem. |
|||
Dart Drop Test | 100 g | 0.221 lb | |
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 38.1 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |
|||
Dart Drop Test | 100 g | 0.221 lb | gF/50%f; ASTM D1709 |
Braskem LF0720/20AF Blown Film Extrusion Linear Low Density Polyethylene Description: LF0720/21AF is a LLDPE Butene copolymer produced using Unipol process technology. It shows excellent optical properties associated with good balance of mechanical properties, processing.. |