Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 130 g | 0.287 lb | F-50 at 26 in.; ASTM D1709 |
Chevron Phillips 7109BK Linear low density polyethylene blown film resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymer, blow film resin, medium slip, medium antiblock version of 7109Characteristics: good stiffness at thin gauges, good drawdown, low COF, c.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
Iran Petrochemical (PCC) Tabriz 1209AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
M. Holland Company LL102 LLDPE
(discontinued **) Additives: Medium Antiblock, Medium SlipFeatures: Medium Antiblocking, Butene Comonomer, Copolymer, Good Drawdown, Good Processability, Medium SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c).. |
|||
Dart Drop Test | >= 130 g | >= 0.287 lb | ASTM D1709 |
Iran Petrochemical (PCC) Bandar Imam Poliran LH0050 LDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D 1709 A |
Total Finathene® DF 210 HDPE resin
(discontinued **) Applications: Irrigation tape and tubingInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines. |
|||
Dart Drop Test | 130 g | 0.287 lb | (method A); ASTM D1709 |
Petroquimica Triunfo Trithene® TS 8064 LDPE - Packaging Film The Trithene TS 8064 resin is a low-density polyethylene (LDPE) with a medium molecular weight an excellent processability. Furthermore, this product has good mechanical properties, average transpar.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709-98 |
Ipiranga Petrochem LB 0316 LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
SCG Chemicals EL-Leneâ„¢ L1810F Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesContains 1600 ppm slip agent and 1900 ppm antiblocking agentRecommended Applications:Film for heavy duty bag, industrial bag, rice bag, su.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
SCG Chemicals EL-Leneâ„¢ L1810FI Linear Low Density Polyethylene Film Key Characteristics:High gloss and clarityContains 3200 ppm slip agent and 2400 ppm antiblocking agentRecommended Applications:Water-quench blown film for general purpose bags such as vegetable or f.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
SCG Chemicals EL-Leneâ„¢ L2009F Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains 1000 ppm slip agent and 700 ppm antiblocking agentR.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
SCG Chemicals EL-Leneâ„¢ L2009FA Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains no slip agent and antiblocking agentRecommended App.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
SCG Chemicals EL-Leneâ„¢ LD1905FA Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains 1000 ppm slip agent and 700 ppm antiblocking agentR.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ISO 7765-1 |
Total LLDPE LL 1820 H Linear Low Density Polyethylene - Blown Film LL 1820 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 H can be processed at high o.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ISO 7765-1 |
Total LLDPE LL 1820 Linear Low Density Polyethylene - Blown Film LL 1820 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 can be processed at high outpu.. |
|||
Dart Drop Test | 130 g | 0.287 lb | F50; ASTM D1709 |
Total Lotrene® Q2018C Linear Low Density Polyethylene, Blown Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Dart Drop Test | 130 g | 0.287 lb | F50; ASTM D1709 |
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Dart Drop Test | >= 130 g | >= 0.287 lb | 20µm film, HDPE |
Total HT 514 MDPE film Finathene® HT 514 is a medium density polyethylene produced by the slurry loop low pressure polymerization process. Finathene® HT 514 can be used alone, blended or coextruded in a wide variety of .. |
|||
Dart Drop Test | 130 g | 0.287 lb | F50; ASTM D1709 |
Total Lotrene® Q2018N Linear Low Density Polyethylene, Cast Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709A |
ExxonMobil Enable™ 27-05HH Metallocene Polyethylene Resin Product Description: Enable 27-05HH is a metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709A |
ExxonMobil Nexxstar™ NX-00328 Low Density Polyethylene Resin Product Description: Nexxstar 00328 is an LDPE grade, which offers good film rigidity combined with very good optical properties. Its primary use is for high performance collation shrunk packaging.A.. |
|||
Dart Drop Test | 130 g | 0.287 lb | Method A; ASTM D1709 |
Dow TUFLIN™ HSE-1003 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-1003 NT 7 is an ethylene-hexene-1 copolymer, design.. |
|||
Dart Drop Test | 130 g | 0.287 lb | g/F50; ASTM D1709 |
Braskem Green PE SLL118/21 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLL118/21 is a LLDPE Butene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties .. |
|||
Dart Drop Test | 130 g | 0.287 lb | gF/50%f; ASTM D1709 |
Braskem LL118/21 Blown Film Extrusion Linear Low Density Polyethylene Description: LL118/21 is a LLDPE Butene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties a.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM-D1709 |
Braskem LL4800N PEBDL Cast Film Extrusion Polyethylene Copolymer LL4800N is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process. It was developed for cast film extrusion. Films obtained with this product show a good processi.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM-D1709 |
Braskem LL6802N LLDPE Blown Film Extrusion Polyethylene Copolymer LL6802N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains processing aid .. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
M. Holland Company LL106 LLDPE
(discontinued **) Additives: Antiblock, SlipFeatures: Unspecified Antiblocking, Hexane Comonomer, Copolymer, Good Drawdown, Good Processability, Unspecified SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c) 2.2.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D 1709 A |
Total Finathene® HL 328 HDPE resin
(discontinued **) Applications: Specialty merchandise bags, millinery/notion bags, mailing envelopes, heavy-duty shipping sacks, shrink films, fresh cut produce packaging, coextrusionInformation provided provided by .. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
ExxonMobil Enable™ 27-05HH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 27-05HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Dart Drop Test | 130 g @Thickness 0.0400 mm |
0.287 lb @Thickness 0.00157 in |
ISO 7765-1 |
Borealis Borstar® FB4370 Medium Density Polyethylene Borstar® FB4370 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Applications: Borstar® FB4370 has been developed especially for ap.. |