Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Elmendorf Tear Strength, MD = 178 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
Reliance Industries LLDPE film - Inorganic salt based film
Information provided by Reliance Industries
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
ASTM D1922
Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film
The Trithene® TS 4016 resin is a mixture of low-density polyethylene (LDPE) with linear low-density polyethylene (LLDPE) designed to meet the needs of the technical films segment for the use of aut..
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
ASTM D1922
SABIC HP0722N Low Density Polyethylene for Blown Film
Product Description: HP0722N is a Low Density Polyethylene grade suitable for producing medium duty films and contains no slip or antiblock additives. It yields good toughness and optical properti..
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
ASTM D1922
Lotte Chemical Titan TITANEX® LF1041 Linear low density polyethylene resin  (discontinued **)
LF1041 is a pelleted linear low density polyethylene resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown film extrusion which offers outstanding toughne..
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
ASTM D1922
Lotte Chemical Titan TITANEX® LF1043 Linear low density polyethylene resin  (discontinued **)
LF1043 is a pelleted linear low density polyethylene resin formulated with antioxidant, and antiblock agent. This product is used for blown film extrusion which offers outstanding toughness, extrud..
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
ASTM D1922
Lotte Chemical Titan TITANEX® LF1044 Linear low density polyethylene resin  (discontinued **)
LF1044 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding toughness, extrudability and draw down..
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
ASTM D1922
Lotte Chemical Titan TITANEX® LF2021 Linear low density polyethylene resin  (discontinued **)
LF2021 is a pelleted linear low density polyethylene resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown and cast film extrusion which offers outstandin..
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
ASTM D1922
Lotte Chemical Titan TITANEX® LF2024 Linear low density polyethylene resin  (discontinued **)
LF2024 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and ..
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
ASTM D1922
Lotte Chemical Titan TITANEX® LF2824 Linear low density polyethylene resin  (discontinued **)
LF2824 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and ..
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
ASTM D1922
Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film
The Trithene® TX 3003 resin is a low-density polyethylene (LDPE) with high molecular weight, presenting excellent mechanical properties. The product provided elevated gloss and transparency, adding..
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
ASTM D1922
Lotte Chemical Titan TITANLENE® LDF250YZ Low density polyethylene
LDF250YZ is a low density polyethylene resin for film extrusion. LDF250YZ has no slip and anti-block additives. LDF250YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u..
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
Dow AFFINITY™ PL 1880 Polyolefin Plastomer
AFFINITY® PL 1880 polyolefin plastomer is an ethylene alpha-olefin resin designed for use in a variety of demanding packaging applications including high-speed, form-fill seal products. AFFINITY PL..
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
ASTM D1922
NOVA Chemicals Sclair® 11M1 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, strength and toughness.Applications: Co-extrusion.Data provided by the manufacturer.
Copyright © lookpolymers.com All Rights Reserved