Reliance Industries LLDPE film - Inorganic salt based film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer Reliance Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries LLDPE film - Inorganic salt based film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Reliance Industries
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 510 %
510 %
Film Elongation at Break, TD 620 %
620 %
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
Elmendorf Tear Strength, TD 19.0 g/micron
483 g/mil
Dart Drop 4.60 g/micron
117 g/mil
Film Tensile Strength at Break, MD 23.0 MPa
3340 psi
Film Tensile Strength at Break, TD 16.0 MPa
2320 psi
Optical Properties Metric English Comments
Haze 44 %
44 %