Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 23 I Butene Copolymer Linear Low Density Polyethylene Flexirene FG 23 I is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 I represents the version of Flexirene FG 20 I.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 30 Low Density Polyethylene - Blown Film Extrusion Riblene FF 30 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 30 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
NOVA Chemicals Novapol® TD-9022-D Super Hexene Film Resin Excellent dart impact, High strength, High toughnessApplications: Retail trash bagsAdditives: Process stabilizer, Slip/antiblockFilm properties are typical of blown film extruded at a blowup ratio o.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-0119-F Hexene LLDPE Film Resin Film Properties. Features: High strength and toughness, low gel count.Applications: Stretch wrap, blend resin.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 23 F Butene Copolymer Linear Low Density Polyethylene Flexirene FG 23 F is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 F represents the version of Flexirene FG 20 F.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
NOVA Chemicals Sclair® 11Q4 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity, good seal characteristics.Applications: Liquid packaging, specialty blending, general purpose sealant.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
Eastman 1810F Polyethylene
(discontinued **) Polyethylene 1810F is a fractional-melt low-density formulation with no slip or antiblock. It is suggested for film applications requiring high impact strength, high tear strength and very good opt.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
Eastman D4004-F Polyethylene
(discontinued **) Polyethylene D4004-F is a fractional melt formulation designed for film applications. It is suggested for applications requiring toughness, clarity, high strength, and for blending with LLDPEList o.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
Eastman D4028-F Polyethylene
(discontinued **) D4028-F is a low density formulation which contains high antiblock. It is suggested for film applications that require reasonable clarity. D4028-F meets the requirements of FDA regulations at 21 CF.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil Escorene® LD-104 LDPE Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer packaging film resin with excellent clarity and good stiffness. It is excellent either blown film or chill roll casting equipment. I.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
LyondellBasell Montell 16501F4 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets F.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
LyondellBasell Petrothene® NA345009 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
LyondellBasell Petrothene® NA345196 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ISO R527-1 |
Iran Petrochemical (PCC) 2100TN00 Low Density Polyethylene LDPE 2100TN00: Heavy duty film suitable for application in shrink hoods, industrial sacks, heavy duty carrier bags and liners.Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
Iran Petrochemical (PCC) LL0220KJ Linear Low Density Polyethylene LL0220KJ are linear low density polyethylene copolymers containing butane-1 as the comonomer.Applications: shipping sacks, carrier and garbage bags, consumer packaging, high clarity film, agricultu.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ISO R527-1 |
Iran Petrochemical (PCC) 2004TC37 Low Density Polyethylene LDPE 2004TC37: Light duty film used for very thin films requiring good optical properties for general packaging.Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ISO 527 |
Iran Petrochemical (PCC) LF0190 Low Density Polyethylene LF01090 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: general pupose film and for aminati.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
Total Lotrene® Q1018N Linear Low Density Polyethylene, Blown Film Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
Total Lotrene® Q1018H Linear Low Density Polyethylene, Blown Film Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
Total Lotrene® Q2018N Linear Low Density Polyethylene, Cast Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LD 105.30 Very High Clarity Packaging Film Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LD 105.BR Very High Clarity Packaging Film Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LDPE LD 185BW Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LDPE LD 185GE Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
Eastman D4032-F Polyethylene
(discontinued **) D4032-F is a low density, fractional-melt formulation which contains no slip and medium antiblock. It is designed for film applications requiring exceptional toughness, such as in heavy-duty shippi.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil Escorene® LD-332 EVA Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 1% vinyl acetate copolymer packaging film resin. Film made from LD-332 offers improved impact strength and heat sealability compared to homopolym.. |
|||
Film Tensile Strength at Yield, TD | 11.0 MPa | 1600 psi | ASTM D882 |
Eastman D4052-F Polyethylene
(discontinued **) D4052-F is a fractional-melt low density formulation with low slip and low antiblock. It is suggested for film applications requiring impact strength, outstanding clarity, and good tear resistance... |