Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Clearflex® FG 106 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FG 106 are characterized by .. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T CLH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T CLH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CLH 108 show e.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
SABIC 318B Linear Low Density Polyethylene for Cast Film Product Description: 318B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0424-A LDPE Foam Resin Good stiffness, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blown film extr.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0323-A LDPE Film Resin Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Food wrap, consumer packaging, liners, blends with LLDPE.Data provid.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0718-A LDPE Film Resin Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical .. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y320-D Fractional Melt LDPE Film Resin Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® PF-Y821-BP Butene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, intended for narrow die gaps.Applications: General purpose packaging, bags requiring moderate clarity, bread bags.Data provided by the m.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D 882 |
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 25 Micron Film FPs021-F complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
SABIC HP0322N Low Density Polyethylene for Blown Film Product Description: HP0322N is a Low Density Polyethylene grade suitable for producing heavy duty films and contains no slip or antiblock additives. It yields outstanding toughness and optical pr.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | at 2% offset; ASTM D882 |
ExxonMobil LL 3301.63 Premium High Strength Film Resin
(discontinued **) LL 3001 resins are hexene copolymer LLDPE film resins. Films produced from this resin have excellent tensile, toughness, and drawability properties. LL 3001 resins are available with blown film addi.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
Westlake Hifor SC74561-F Clear (Voridian) Polyethylene Film, Using Energx Technology Services
(discontinued * VORIDIAN HIFOR CLEAR SC74558-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and low antiblock additives. Films produced with t.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
Eastman 1925F Polyethylene Film
(discontinued **) Polyethylene 1925F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y819-A LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, shrink film, blends with LLDPE, small dia.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® PF-0118-F Butene LLDPE Film Resin Film Properties. Features: Toughness and strength.Applications: Stretch wrap, blend resin, industrial packaging.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D 882 |
NOVA Chemicals Novapol® PF-0218-E Butene Copolymer LLDPE Film Resin PF-0218-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
Iran Petrochemical (PCC) LL 18XF5 N Linear Low Density Polyethylene LL 18XF5 N is a terpolymer of ethylene, propylene and butene-1 for high film strength applications, especially heavy duty shipping sacks, ice bags, frozen food bags, potato bags, and agriculture fil.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ L1810F Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesContains 1600 ppm slip agent and 1900 ppm antiblocking agentRecommended Applications:Film for heavy duty bag, industrial bag, rice bag, su.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ L1810FI Linear Low Density Polyethylene Film Key Characteristics:High gloss and clarityContains 3200 ppm slip agent and 2400 ppm antiblocking agentRecommended Applications:Water-quench blown film for general purpose bags such as vegetable or f.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ LD1905F Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE, LLDPEContains 1500 ppm slip agent and 2600 ppm antiblocking agentRecommended Applications:General purpose bagVeg.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
Chevron Phillips MarFlex® D139DK Metallocene Linear Low Density Polyethylene, Blown Film This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
Chevron Phillips MarFlex® D139FK Metallocene Linear Low Density Polyethylene, Blown Film This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | |
Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045 Polyethylene resin is a premier film resin for heavy duty applications. It complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications. The regulation sh.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | |
Dow DOWLEX™ 2045A Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2045A Polyethylene blown film extrusion resin is a premier film resin for heavy duty applications. It is utilized where improved thermal stability over a broader range of processing conditi.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | |
Dow DOWLEX™ 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245D Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245D resin is used where improved thermal stability over a broad range of processing conditions is nece.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
Westlake Hifor SC74560-F Clear Polyethylene
(discontinued **) Hifor Clear Polyethylene SC74560-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and medium antiblock additives. Films produc.. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Sclair® 11B4 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Sclair® 11M1 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, strength and toughness.Applications: Co-extrusion.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, TD | 10.0 MPa | 1450 psi | ASTM D882 |
Eastman D4036-F Polyethylene
(discontinued **) D4036-F is a low density formulation with high slip and high antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial and gener.. |