Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 4.60 GPa | 667 ksi | Calculated |
Premix Premi-Glas® 1200-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-20 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | Calculated |
Premix Premi-Glas® 1200-22 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | Calculated |
Premix Premi-Glas® 1200-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | Calculated |
Premix Premi-Glas® 1200-30 Polyester SMC Premi-Glas® 1200-30 is a fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck and Marine body panels and interior structural components where smooth flat surfac.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | Calculated |
Premix Premi-Glas® 1200H-15 Polyester SMC Premi-Glas® 1200H-15 is a 15% fiberglass-reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94 HB flame re.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | Calculated |
Premix Premi-Glas® 1200H-22 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | Calculated |
Premix Premi-Glas® 1200H-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | Calculated |
Premix Premi-Glas® 1240-15 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-15 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | Calculated |
Premix Premi-Glas® 2103-20 CR-SX Fiberglass Reinforced Thermoset BMC Premi-Glas® 2103-20 CR-SX is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regu.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | Calculated |
Premix Premi-Glas® 2103-22 CR-SX-HT Fiberglass Reinforced Thermoset BMC Premi-Glas® 2103-22 CR-SX-HT is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL .. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | Calculated |
Premix Premi-Glas® 2103-25 CRSX Polyester BMC Premi-Glas® 2103-25 CR-SX is a 25% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | Calculated |
Premix Premi-Glas® 2200-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | Calculated |
Premix Premi-Glas® 2203-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | Calculated |
Premix Premi-Glas® 2204-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | Calculated |
Premix Premi-Glas® 2205-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | Calculated |
Premix Premi-Glas® 3101-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-15 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | Calculated |
Premix Premi-Glas® 3200-30 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-30 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | calculated |
BASF Capron® GR40 HS 40% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR40 HS is a heat stabilized 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stabil.. |
|||
Shear Modulus | 4.60 - 5.00 GPa | 667 - 725 ksi | Average value: 4.73 GPa Grade Count:3 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | in plane |
Menzolit Menzolit® SMC 0170 Unsaturated Polyester UP SMC 0170 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | in plane |
Menzolit Menzolit® SMC 0390 Unsaturated Polyester UP SMC 0390 is a standard low profile SMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surfac.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | in plane |
Menzolit Menzolit® SMC 0410 Unsaturated Polyester UP SMC 0410 is a Premium Class-A SMC for on-line painted exterior body applications on cars developed with CCC technology. These compounds mould to parts with excellent surface quality for on-line pain.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | in plane |
Menzolit Menzolit® SMC 1500 Unsaturated Polyester UP SMC 1500 is a special SMC for applications calling for high continuous service temperature. The glass level has been selected to combine good mouldability with good strength and stiffness properties.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | in plane |
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP SMC 2600 is a special SMC with electrically conductive properties. Because of its conductivity, SMC 2600 is antistatic and prevents build-up of electrical charges on the surface. Despite of its cond.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | in plane |
Menzolit Menzolit® SMC 0150 Unsaturated Polyester UP SMC 0150 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | in plane |
Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP SMC 0160 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets .. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | in plane |
Menzolit Menzolit® SMC 0290 Unsaturated Polyester UP SMC 0290 is a specially formulated SMC processable by injection moulding. The gentle production process prevents the fiber from any damage. Parts made of SMC 0290 reach higher levels of strength and.. |
|||
Shear Modulus | 4.60 GPa | 667 ksi | in plane |
Menzolit Menzolit® SMC 0300 Unsaturated Polyester UP SMC 0300 is a low shrink standard SMC providing improved surface quality, reduced shrinkage and warpage. Typical fields of applications are mechanical engineering and electrical industry, where impr.. |
|||
Shear Modulus | 4.60 GPa @Temperature 23.0 °C |
667 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-6 Curing Cyanate Resin, M40J Fiber Information provided by HexCel |
|||
Shear Modulus | 4.60 GPa | 667 ksi | calculated |
BASF Capron® GR40 40% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR40 is a 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is also ava.. |