Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.20 GPa | 609 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 GF 5 FRA 5 Polyamide 6, 5% Glass Fiber, Halogen Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 5% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C, .. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | Type 1B, 50mm/min; ISO 527-1/2:1993 |
Nylacast Nylube MO Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), MoS2 Filled The combined Nylube lubrication system incorporating fine particles of molybdenum disulphide provides enhanced load bearing capabilities while retaining Nylube's excellent frictional characteristics.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | MD; DIN EN ISO 527 |
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | CD; DIN EN ISO 527 |
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527-1/-2 |
Quadrant EPP Duratron® PAI T4203 PAI, unfilled, extruded (ISO Data) Duratron T4203 PAI offers the best toughness and impact strength of all Duratron PAI grades. This extruded Duratron PAI grade is very popular for precision parts in high-tech equipment. In addition,.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | |
Radici Radilon® A ERV1906LK (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527-2/1A |
Radici Raditer® B RVA 100 Polybutylene Terephthalate with 10% Glass fiber Raditer® B RVA is a range of glass fiber reinforced Polybutylene terephthalate blends for injection molding, with excellent dimensional stability, low warpage and good surface aspect.Information pr.. |
|||
Tensile Modulus | 4.20 GPa @Thickness 0.100 mm |
609 ksi @Thickness 0.00394 in |
TD; ISO 527 |
Victrex® APTIV® 1102-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 20% Mineral Filled APTIV PEEK 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance application.. |
|||
Tensile Modulus | 4.20 GPa @Temperature 23.0 °C |
609 ksi @Temperature 73.4 °F |
ISO 527 |
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, .. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527-2 |
NOVA Chemicals Dylark® 520XT Glass Reinforced Engineering Resin Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri.. |
|||
Tensile Modulus | 4.20 GPa @Temperature 23.0 °C |
609 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**) Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ASTM D638 |
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | conditioned, 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® BKV 230 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fiber, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Asia Pacific) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 7062 PBT+PET (Europe-Africa-Middle East) Valox 7062 is Mineral filled PBT injection molding grade. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP AF002 ABS LNP THERMOCOMP* AF002 is a compound based on ABS resin containing 10% Glass Fiber. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp AF0029 ABS (Europe-Africa-Middle East) LNP* THERMOCOMP* AF0029 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features include: Flame Retardant.This data was supplied by SABIC-.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp WB006 PBT LNP* Thermocomp* WB006 is a compound based on Polybutylene Terephalate resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 126K6 Nylon 6, 30% Glass Filled SAXAMID 126K6 is a 30% glass beads filled polyamide 6 injection-molding-grade. It is characterized by dimensional stability, low warpage and good surface quality.Information provided by SAX Polymers.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 226K6 Nylon 6.6, 30% Glass Beads SAXAMID 226K6 is a polyamide 6.6 injection-molding-grade filled with 30% glass beads. It is characterized by optimized shrinkage properties.Information provided by SAX Polymers |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP AF002XXC ABS LNP THERMOCOMP* AF002XXC is a compound based on ABS resin containing 10% Glass Fiber. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527-1/-2 |
Covestro Makroblend® DP 7665 Polycarbonate + PET, Mineral Filled Impact Grade Developmental productISO 7792-1-PC/PET,MHPR,-030,MD20(PC+PET)-blendsimpact modifiedInjection molding grade 20 % mineral filledPreprocessingMax. Water content |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 MR 209 HWCP Mineral Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 50mm/min; ISO 527-1 |
Denka CL-430 Transparent Resin Polymer (MABS) ABS "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® B3 GF 20 (2470) PA 6 Conditioned, 20% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ASTM D638 |
Gharda Chemicals G-PAEK™ 1200P Ultra High Performance PEK Polymer Product Details: Ultra High performance thermoplastic material, unreinforced Poly Aryl Ether Ketone (G-PAEK), semi-crystalline, coarse powder for extrusion compounding, FDA food contact compliant, .. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
Victrex® HT™ P45PF Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact compliantInfor.. |