Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.30 GPa | 479 ksi | |
Plastcom SLOVAMID 6 GF 20 PA6, 20% glass beads FeaturesNearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical properti.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527-1/-2 |
Quadrant EPP Ertacetal® H POM-H, extruded (ISO Data) Ertacetal H is Quadrant’s homopolymer acetal grade. It offers a higher mechanical strength, stiffness, hardness and creep resistance as well as a lower thermal expansion rate and often also a bette.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 500ECR PC Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 500R PC (Europe-Africa-Middle East) LEXAN 500R is a medium viscosity, 10% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and excellent impact pe.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 5271/2 |
Radici Radilon® S 37FL T Nylon 6 Radilon® S (homopolyamides) are normally used in cast and blown extrusion for the production of packaging films. Radilon® S grades can be extruded to a thickness varying from 20 mm to 100 mm.Appl.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Asia Pacific) 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP FARADEX NX96302 PC+ABS LNP* FARADEX* NX96302 is a compound based on PC+ABS resin containing Stainless Steel Fibers. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527 |
Nilit FRIANYL B63 W-KV10 Nylon 6 for injection molding, 10% glass ball reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HF500R PC (Europe-Africa-Middle East) LEXAN HF500R is an easy flow, 9% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and impact performance. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP IBI16 PA 6/12 LNP LUBRICOMP* IBI16 is a compound based on Nylon 6/12 resin containing 30% Glass Bead, 2% Silicone. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1010RF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.This data was supplied by SABIC-IP for the Americas reg.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 8015 PEI (Asia Pacific) High flow Polyetherimide blend. Meets FAR 25.853 and OSU 100/100 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM DU319 PEI Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK) AvaSpire® AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527-1/-2 |
Styrolution Polystyrol 165 H GR 2 PS Description: Polystyrol 165 H is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.Applications: In blends with high impact Polystyrene or Styrolux; thermo.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527 |
Styrolution Terblend® N NG-02 UV ABS / PA, 8% Glass filled Terblend N NG-02 UV is an 8% glass fiber reinforced (UV stabilized) ABS/PA blend with enhanced dimensional stability and rigidity.High dimensional stabilityEnhanced rigidityEnhanced softening temper.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP NF001XXX PC+ABS LNP* THERMOCOMP* PCA-F-1001 is a compound based on PC+ABS resin containing 5% Glass Fiber. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527-1/-2 |
Covestro Bayblend® ET 1100* Polycarbonate + ABS, Mineral Filled As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ HMU 301 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for high heat and discoloration resistance, good surface finish, and detergent resistance for electrical appliances such as w.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 300PE BK602 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE BK602 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration .. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® PC690 NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC690 is a low viscosity acetal homopolymer developed for parts requiring high precision molding in the healthcare indus.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527-1/-2 |
DSM Stanyl® TW341 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | |
BASF Polystyrol® 158 K Polystyrene (Global) Heat-resistant, rapid freezing general-purpose grade. Suitable for expanded film and for blending with Styrolux and impact-modified Polystyrol in heat contact applications (e.g. coffee cups).Data w.. |
|||
Tensile Modulus | 3.30 GPa @Temperature 23.0 °C |
479 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It has improved dimensional stability, high strengt.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 1 mm/min |
Arkema Group Oroglas® V 044 Acrylic, Extrusion Grade
(discontinued **) OROGLAS V 044 is an extrusion grade offering good compromise between physical properties and thermal resistance.OROGLAS V 044 is recommended for extrusion of profiles, tubes and sheets.ISO data prov.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 1 mm/min |
Arkema Group Oroglas® V 920 T Acrylic, Injection Molding Grade
(discontinued **) OROGLAS V 920 T is an injection molding grade with an improved thermal resistance HDT A ( 1.82 MPa ) = 96°c without any adverse effect on mechanical and optical properties.The processing of OROGLAS.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527 |
Grupo Repol Dinalon® B2S35 V2-7035 PA6 High Viscosity, V2 Halogen Free, RAL 7035 Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |