Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.62 GPa | 380 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding MR200 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CX3222ME PC+ABS Cycoloy* resin grade CX3222ME is an extrudable & thermoformable PC/ABS blend with non brominated and non chlorinated flame retardant systems. Key features of low gloss and good impact make it ideal .. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | ASTM D638 |
Manifattura Cattaneo VESPEL® SP21 Polyimide Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | |
Ineos ABS Lustran® 348 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | ASTM-D638 |
Ineos ABS Lustran® ABS 349 Lustran® ABS 349 is a high-gloss, medium-impact injection molding resin that has been specially formulated for excellent surface lubricity using internal additives. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | ASTM D638 |
Fiberfil® PP-60/CC/30 Polypropylene Homopolymer, 30% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer LNP* LUBRICOMP* KL001 is a compound based on Acetal Copolymer resin containing 5% PTFE. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Europe-Africa-Middle East) LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL N850 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
Tensile Modulus | 2.62 GPa @Thickness 3.20 mm |
380 ksi @Thickness 0.126 in |
Injection Molded; ASTM D638 |
Styron EMERGEâ„¢ 7700 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7700 Advanced Resin is an ignition-resistant PC/ABS blend that contains no chlorine for bromine additives. It has superior processability for injection molding applicat.. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | ASTM D638 |
Ensinger HYDEX® 4101L Polybutylene Terephthalate (PBT) HYDEX® 4101 & 4101L (lubricated) is a very stable chemical compound that can withstand high impact without deterioration. It is approved for direct contact with food by the FDA and is ideal for ma.. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | ASTM D638 |
Ensinger Tecaform™ Acetal Copolymer - Extruded Products (POM) Tecaform™ is a semi-crystalline thermoplastic offering high strength, stiffness and toughness. It is resistant to hot water, hydrocarbons and solvents, and it posses good bearing and wear properti.. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | ASTM D-638 |
Axiall 8247 Clear 34 Rigid PVC, Extrusion, Clear 34 Georgia Gulf 8247 Clear 34 is a rigid PVC pellet compound suited for applications where transparency is important. It is widely used for clear profiles such as furniture trim, shower door and prote.. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ CPVC LC500 Polyvinyl Chloride, Chlorinated (CPVC) Geon LC500 CPVC is an extrusion grade rigid compound. It is designed for applications where enhanced resistance at elevated temperatures is needed. LC500 demonstrates ease of processing with excelle.. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | ASTM D-638 |
Axiall 3650 Rigid PVC, Extrusion Georgia Gulf 3650 is a special purpose rigid PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChemical Resistan.. |