Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.50 GPa | 363 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® S701 ABS (Europe-Africa-Middle East) CYCOLAC S701 is a new developed ABS providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an excellent fit in appli.. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® S705 ABS (Europe-Africa-Middle East) CYCOLAC S705 is a new generation ABS plating grade, offering semi high heat with a good property balance for impact and flow. CYCOLAC S705 demonstrates excellent electroplatability and a good therma.. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers OpteSTAT™ NC PPS 7010 Polyphenylenesulfide based Carbon Nanotube Compound Material resistivity can be tailored to the application, while retaining the physical and thermal properties of the base polymer. Applications include components of disk drives, business machines or.. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY201 PC+ABS (Europe-Africa-Middle East) Cycoloy* CY201 is an industrial quality PC+ABS Flame Retardant grade for injection moulding applications. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | ISO 527 |
Nilit FRIANYL B63 H-TF20 Nylon 6 for injection molding, 20% PTFE lubricated Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics GELOY HRA170 ASA (Europe-Africa-Middle East) GELOY HRA170 is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour .. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | ISO 527-1,2 |
Qualchem Danamid FEH Polyamide 6 Heat stabilized type polyamide, for long-lasting use at 120-130°CInformation provided by Qualchem Zrt. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP AX98567H ABS LNP* COLORCOMP* AX98567H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP FARADEX DS0036I PC (Europe-Africa-Middle East) LNP* Faradex* DS0036I is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel Fiber. Added features of this material include: High Impact, Flame Retardant, Non-Bromin.. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | 1 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® ABS 377 Plating, Injection Molding Grade |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | 1 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® ABS 450 Injection Molding Grade Lustran® ABS 450 has medium impact strength, high flow, and is injection molding grade. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 315 Z H2.0 901510 Nylon 6, 15% Glass Fiber PA 6 extrusion- and blow molding-grade with 15% glass fibers, branched/structural viscosity, elastomer-modified, good heat-ageing resistance, dry-impact modifiedApplication Examples: air intake hose.. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 52G3 MZ25 PA6, Conditioned Description: Flame retardant polyamide PA6 reinforced with mineral filler, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: This phosph.. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 175 PBT (Europe-Africa-Middle East) Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® V2105U PBT Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | ISO 527 |
Styrolution Novodur® E211 ABS Novodur E211 is a high heat extrusion grade and suitable for blow moldingInformation provided by Styrolution |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL NH5110E PPE+PS (Europe-Africa-Middle East) NORYL NH5110E is a flame retardant, non halogenated, impact modified extrusion grade. Developed for low beard-growth, with a Vicat B/120 of 138 Deg C, according to ISO 306 and a UL-94 rating of V1@ .. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | 1 mm/min; ISO 527-1,-2 |
Covestro Bayblend® ET3036 FR PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Extru.. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | ISO 527-1/-2 |
DSM Akulon® K222-KWGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | 1mm/min; ISO 527-1 |
Denka MALECCA K-100 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | ISO 527 |
Eurotec® Tecodur® PB30 NL PBT, unfilled, natural, high viscosity, extrusion grade Information provided by Eurotec® |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | ISO 527 |
Eurotec® Tecodur® PB70 NL PBT medium viscosity Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | |
Plastcom SLOVAMID 6 LI LS PA6, improved strength, light stability FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme.. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | |
Plastcom SLOVASTER® B2 BT PBT, basic type FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, Conditioned Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr.. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | |
BASF Luranyl® KR 2451/3 Polyphenylene Ether + Styrene-Butadiene Blend Especially easy flowing grade containing halogen-free, flame-retardant; mainly used for housings for electrical equipment and in the electronics sector.Data was collected by ISO methods and provided.. |
|||
Tensile Modulus | 2.50 GPa | 363 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Asia Pacific) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |