Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.21 GPa | 321 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific) Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® FR15U ABS (Europe-Africa-Middle East) CYCOLAC FR15U is a flame retardant ABS with good processability and good indoor UV properties. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer (Asia Pacific) Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer (Asia Pacific) Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with .. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with .. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer (Asia Pacific) Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Asia Pacific) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer (Asia Pacific) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPX4EU PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPX4REU PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) .. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP D1000P PC LNP* COLORCOMP* D1000P is an unfilled Polycarbonate. Added feature of this grade is: Exceptional Processing. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP D1000P PC (Asia Pacific) LNP* Colorcomp* D1000P is a compound based on Polycarbonate resin containing Unfilled Custom Color. Added features of this material include: Exceptional Processing. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXE1413T PC Copolymer Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP COLORCOMP DX04401H PC LNP* COLORCOMP* DX04401H is an unfilled Polycarbonate. Added feature of this grade is: Healthcare. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON SD000 PA12 LNP* STAT-KON* SD000 is an unfilled Nylon 12 compound. Added feature of this grade is: Electrically Conductive. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | ASTM Data |
Styron CALIBRE™ MEGARAD 2080 15 Polycarbonate, Gamma Radiation Resistant CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate Resin Overview: CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate resin provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to hi.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | ASTM Data |
Styron Magnum™ 2645 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | ASTM Data |
Styron Magnum™ 545 ABS, General Purpose MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | ASTM Data |
Styron CALIBRE™ 603 5 Polycarbonate, Branched CALIBRE® 603 is a branched polycarbonate resin and is equipped with a mold release and a UV stabilization package. CALIBRE 603 resins exhibit an excellent property balance of high clarity, high m.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | ASTM Data |
Dow Retain® ABS 7490 ABS Data provided by Dow Chemical. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with .. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | ASTM Data |
Styron Magnum™ 3490 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |