Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.45 GPa | 210 ksi | |
Plastcom SLOVALEN PC 16 FRD 1 PP, flame retardant Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | |
Plastcom SLOVALEN PQ 83 T 20 PP, 20% mineral filling FeaturesModified PP for injection moulding with the content of 20% mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased .. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | 1 mm/min; ISO 527 |
Polimeri Europa Edistir ICE R 830D Polystyrene Environmental stress cracking resistant (ESCR) HIPS. ICE PD R 830D combines high impact strength with an improved chemical resistance to oils, fats and chemical agents, such as detergents for both i.. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | ISO 527 |
Polimeri Europa Edistir® PD ICE S 900 High Impact Polystyrene - Very High ESCR Very high environmental stress cracking resistant (VH ESCR) HIPS.ICE S 900 exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents, and in particular to cyclopent.. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | ISO 527-1/-2 |
Quadrant EPP Fluorosint® 207 PTFE + mica, compression moulded (ISO Data) This material has a food contact compliant composition which, in combination with the good mechanical performance, dimensional stability, sliding and wear properties and inherent outstanding chemica.. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | |
Radici Radilon® CA HS (cond.) Nylon 66/6 Radilon® CA is a range of polyamide 66/6 copolymers obtained through the polymerization of hexamethylendiamine, adipic acid and caprolactam.Information provided by Radici group. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-1000 Polypropylene Block-Copolymer INNOPOL® CS 2-1000 is a polypropylene block-copolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-1000 is developed for producing injection molded automo.. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-9000 MA N Polypropylene Copolymer INNOPOL® CS 2-9000 MA N is a high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA N is developed for producing injection molded automotive components.All information provide.. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | ISO 527-2 |
Total PPH 4030 Polypropylene Homopolymer Polypropylene PPH 4030 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4030 has been designed for the production of BOPP film with the tenter frame process. Th.. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | ISO 527-2 |
Total PPH 4060 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4060 is homopolymer.ApplicationATOFINA Polypropylene PPH 4060 is specially suitable for tape extrusion for woven applications and for extrusion thermoforming. PPH 4060 is.. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | ISO 527-2 |
Total PPH 6080 Polypropylene Homopolymer, Cast Film Polypropylene PPH 6080 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH.. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ CNU 015 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with good stiffness/toughness balance, low odor and emissions, designed for automotive interior applications. Availability: Africa & M.. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | 1 mm/min |
Arkema Group Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Dry) Designation ISO 1874-PA12,MR,14-010Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. mold-release agent... |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | |
BASF Novolen® 1100 H Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | |
BASF Novolen® 1102 H Polypropylene Grade with high processing stability for packaging tapes, film tape, fibrillated film, monofilaments, thermoformed and blow molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | ASTM D638 |
Americas Styrenics EB6755 High Impact Polystyrene Product CharacteristicsGood Environmental Stress Crack Resistance (ESCR)Good practical toughnessDeep draw thermoforming capableGood low temperature impactFood Contact CompliantTypical ApplicationsPa.. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | 1 mm/min |
Arkema Group Rilsan® BECN TL Nylon 11, Sheathing Grade (Dry) Designation ISO 1874-PA11,KHL,12-010Rigid grade for sheathing of wires and cables. Available color: natural. Light and heat stabilized.High abrasion resistance. Well adapted melt viscosity. Ability .. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | ISO527-2 |
ExxonMobil PP1364E2 Polypropylene Homopolymer Product Description: A medium melt flow homopolymer resin suitable for masterbatch carrier and other compounding applications and for the molding of garden furniture, caps and other consumer produc.. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | |
BASF Novolen® 1102 L Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.45 GPa | 210 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Elastamax® HTE 2101 Thermoplastic Elastomer - PVC/TPU
(discontinued **) Description/Features:InteriorUL 94 V0Applications:General PurposeCustom Profiles-ComplexProcessing Method:Extrusion-Single ScrewInformation provided by PolyOne Corporation. |