Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.1 GPa | 1750 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ SF-30GF/15T Polyphenylene Sulfide (PPS) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 12.1 GPa | 1750 ksi | 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® AT-15CF/000 BLACK Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 12.1 GPa | 1750 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ NY-20CF/000 BLACK Polyamide 6 (Nylon 6) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Tensile Modulus | 12.1 GPa | 1750 ksi | ISO 527-1/-2 |
Lanxess Durethan® DP BM 65 X FM30 901510 Nylon 6, 65% Mineral + Glass Fiber PA, injection molding and hybrid grade based on PA 6, 65% mineral/glass fibers, UL 94V-0 at 1.2 mm, reduced cycle times (easy flow), Thin wall application, free from halogen and phosphorous, low smo.. |
|||
Tensile Modulus | 12.1 GPa | 1750 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP UX05051 PPA (Europe-Africa-Middle East) Internally lubricated Polyphthalamide compound, containing Glass Fiber and PTFE. Added features include Heat Stabilized, Flame Retardant and Hot Water Moldable |
|||
Tensile Modulus | 12.1 GPa | 1750 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-8930 HS Polyphthalamide (PPA), 30% Glass Fiber Amodel® A-8930 HS is a 30% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low.. |
|||
Tensile Modulus | 12.1 GPa | 1750 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON ZEF061XC PPO (Europe-Africa-Middle East) LNP* STATKON* ZEF061XC is a compound based on Polyphenyleneoxide resin containing Glass Fiber, Milled Carbon Fiber and Flame Retardant. Added Features include: Electrically Conductive |
|||
Tensile Modulus | 12.1 GPa | 1750 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP OF006 PPS - Linear LNP* THERMOCOMP* OF006 is a compound based on Linear PPS containing 30% Glass Fiber. |
|||
Tensile Modulus | 12.1 GPa | 1750 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP UF007AS PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF007AS is a compound based on Polyphthalamide resin containing Glass Fiber. Added features include Heat Stabilized . |
|||
Tensile Modulus | 12.1 GPa | 1750 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON PX91200 PA 6 LNP VERTON* PX91200 is a compound based on Nylon 6 resin containing Proprietary Fillers. Added features of this material include: High Impact, Structural |
|||
Tensile Modulus | 12.1 GPa | 1750 ksi | ASTM D638 |
Plenco 1508 Polyester, Briquette, Injection Molded PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl.. |
|||
Tensile Modulus | 12.1 GPa | 1750 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 1010GN2-30 NAT/BK37 PA6-GF30 FR(17) 30% Glass Reinforced, Flame Retardant |