Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.0 GPa | 1600 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PC-20CF/15T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 11.0 GPa | 1600 ksi | ASTM D638 |
Premix Premi-Glas® 1200H-10 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:G.. |
|||
Tensile Modulus | 11.0 GPa | 1600 ksi | ISO 527, ASTM D638 |
Nilit Nilamid A G7 FR PH1 35% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G7 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a UL 94 V0 listing 1.5 and a complete yellow card. The formulation has been optim.. |
|||
Tensile Modulus | 11.0 GPa @Temperature 23.0 °C |
1600 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Rynite® RE19051 BK507 PET
(Unverified Data**) Rynite® RE19051 BK507 is a 40% glass and mineral reinforced, flame retardant, polyethylene terephthalate black resin.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 11.0 GPa | 1600 ksi | ISO 527-1/-2 |
Lanxess Pocan® DP 7244 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Tensile Modulus | 11.0 GPa | 1600 ksi | d.a.m.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 11.0 GPa | 1600 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2410EPR PEI 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Tensile Modulus | 11.0 GPa | 1600 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON ZX08301 PPE (Asia Pacific) Stat-Kon* ZX08301 compound is a high heat compounds with ESD safe and low warpage performance suitable for use in Semiconductor Packaging Applications. |
|||
Tensile Modulus | 11.0 GPa | 1600 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, DRY Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used.. |
|||
Tensile Modulus | 11.0 GPa | 1600 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQNH4550 PBT (Europe-Africa-Middle East) Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT.. |
|||
Tensile Modulus | 11.0 GPa | 1600 ksi | ASTM D638 |
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |
|||
Tensile Modulus | 11.0 GPa | 1600 ksi | ASTM D638 |
Ecomass® 1850ZD88 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA6)Information provided by Technical Polymers |
|||
Tensile Modulus | 11.0 GPa | 1600 ksi | ISO 527-1/-2 |
DSM Akulon® K224-HG7 Nylon 6-35% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 11.0 GPa | 1600 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-35/4 PA666-GF35 Product description: Grilon TSG-35/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers. Grilon TSG-35/4 has the following important properties: Good flo.. |
|||
Tensile Modulus | 11.0 GPa | 1600 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-35/4 W black 9832 PA666-GF35 Product description: Grilon TSG-35/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Tensile Modulus | 11.0 GPa | 1600 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G43HSLA BK099 Nylon 66
(Unverified Data**) 43% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G43HSLA BK099 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
Tensile Modulus | 11.0 GPa | 1600 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® HT1V-3 FWA nat PA6T/6I-GF30 Product description: Grivory HT1V-3 FWA natural is a 30 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |
|||
Tensile Modulus | 11.0 GPa | 1600 ksi | ISO 527-2 |
Pasargad Polymer Peyvand Pasamid 3P-H2145B Nylon 66, 45% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Tensile Modulus | 11.0 GPa | 1600 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HT1V-3 HY black 9205 PA6T/6I-GF30 Product description: Grivory HT1V-3 HY black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-3 HY bl.. |
|||
Tensile Modulus | 11.0 GPa | 1600 ksi | |
LATI Laticonther 57 CPG/550 PPA, Glass Fiber Reinforced High thermal conductivity product based on Semi-aromatic polyamide (PPA). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformat.. |