Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.700 GPa | 102 ksi | ISO.527 DIN.53455 |
Omnia Plastica PTFE Polytetrafluoroethylene A Fluoropolymer used mainly for its excellent chemical resistance. It has poor mechanical features. The strain, even under low weight, makes it very suitable as a gasket material.Features:Chemical: .. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | ISO 527-1/-2 |
Quadrant EPP TIVAR® DS PE-UHMW + additives (ISO Data) TIVAR DS is a modified PE-UHMW with extremely high molecular weight. The latter in combination with a particular manufacturing process result in a PE-UHMW grade with superior wear and abrasion resis.. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | ISO 527-1/-2 |
Quadrant EPP TIVAR® H.O.T. PE-UHMW + specific additives (ISO Data) TIVAR H.O.T. [Higher Operating Temperature] is formulated to maintain inherent PE-UHMW key properties over an extended service temperature range, in this way considerably increasing part life in low.. |
|||
Tensile Modulus | >= 0.700 GPa | >= 102 ksi | 2% sec, MD; ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4148B (484H2) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Tensile Modulus | >= 0.700 GPa | >= 102 ksi | 2% sec, MD; ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 6148C (486H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | 1% Secant; ASTM D 638 |
NOVA Chemicals Surpass® IFs932-R Octene SLLDPE Injection Molding Resin IFs932-R complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |
|||
Tensile Modulus | 0.700 GPa @Temperature 150 °C |
102 ksi @Temperature 302 °F |
ISO 527 |
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded
( AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer.. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | MD; ASTM D882 |
Honeywell Aegisâ„¢ H100MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 .. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | |
LyondellBasell Lupolen® 3652 D SW 00413 MDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | |
LyondellBasell Lupolen® 3821 D MDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | DIN 53457 |
Isoflon PEHD 1000 High Density Polyethylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® DP 2325 H3.0 000000 Nylon 66 PA 66, injection molding grade, non-reinforced, elastomer-modified, good heat-ageing resistance, extremely high notched impact strength even at dry state and at low temperatures |
|||
Tensile Modulus | 0.700 - 0.850 GPa | 102 - 123 ksi | MD/TD; ISO 527-3 |
Borealis HD822CF Polypropylene HD822CF is a polypropylene homopolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: food packaging, lamination films, statio.. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | ASTM-D790 |
Polyram PlusTek RD104 Nylon 12, Injection Molding Outstanding flexibility polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 0.700 GPa @Temperature 100 °C |
102 ksi @Temperature 212 °F |
DIN 53457 |
Zell-Metall Engineering Plastics Zellamid 1100 OIL Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces .. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® AZ 3 PA66 Product description: Grilon AZ 3 is a normal viscosity, high impact modified PA66 injection molding grade. Grilon AZ 3 has the following important properties: Excellent toughness at low temperatures.. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® AZ 3/2 PA66 Product description: Grilon AZ 3/2 is an unreinforced and impact modified PA66 injection molding grade. Grilon AZ 3/2 has the following important properties: Excellent toughness at low temperaturesE.. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | In Plane Direction |
Cymat A35620SC 020SS Stabilized Aluminum Foam Description: Cymat A35620SC 020SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.2 g/cm3. The mechanical properties of SAF make it .. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4128 black 9221 PA610 Product description: Grilamid XE 4128 black 9221 is a modified high viscosity Polyamide 610 for extrusion as well as injection molding. A characteristic of tubes made out of this material is the hig.. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | DIN 53 457 |
Hippe PTFE Good chemical resistance. High thermal stability. Flame resistance. Lowest coefficient of friction among all solid plastics. Very good dielectric properties. Very high weathering resistance.Info.. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BRZ 340 H PA6 Product description: Grilon BRZ 340 H is a heat stabilized, high viscosity, impact modified PA6 extrusion grade. Grilon BRZ 340 H has the following important properties:High impact strength at low t.. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® EB 50 H DZ PA6 Product description: Grilon EB 50 H DZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon EB 50 H DZ has the following important properties:.. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | 1 mm/min |
Arkema Group Orgalloy® LE 60LMES Flexible Nylon Alloy (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).ISO data provided by the manufacturer, Arkema. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | 1 mm/min |
Arkema Group Orgalloy® LT 6040ISH Nylon (Conditioned) ISO data provided by the manufacturer, Arkema. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 MCS HI Polyamide 6 - Impact Modified Very high impact resistance, cold impact grade (to -40°C). Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has t.. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | TD |
BASF Ultramid® B36 LN 0.04 mm Cast Film Cold Chillroll Product comes in 2-2.5 mm round pellets.Information provided by BASF |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | 1 mm/min |
Arkema Group Kynar® FLEX 2800 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EG1N, N. ?E7.D.G.B.C,, ? (3.5-7.5)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, impervious.. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | |
Radici Radilon® S ESL128 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 0.700 GPa | 102 ksi | |
LATI Latistat 48/9900-03 EVA Dissipative product based on Ethyl-Vinyl-Acetate (EVA). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |