Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.70 GPa | 1410 ksi | ISO 527 |
Radici Radilon® A GV H0 30P Nylon 66-GF30 Automotive cooling liquid resistant PA66-GF30 grade designed to resist even in more severe operating condition. Indicated as "top of the class" material.Information provided by Radici group. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | |
Radici Radilon® A RV300R (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | ISO 527 |
Gharda Chemicals GATONE™ PEEK, 30% Glass Reinforced
(discontinued **) GATONE™ PEEK grades with glass fiber reinforcements ranging from 10- 40 % are available in natural or desired colors. Custom made grades can be developed to meet specific requirements.CHARACTERISTI.. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG30-FN00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | |
LATI Latigray 82-04 CX/90 PA 12 Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36SXC PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL36SXC is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36SXD PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL36SXD is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East) VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp ZF008 PPO LNP* Thermocomp* ZF008 is a compound based on Modified PPO containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON MV008 PP (Europe-Africa-Middle East) LNP* VERTON* MV008 is a compound based on Polypropylene resin containing Long Glass. Added features include Chemically Coupled. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 3021GH30 NAT PA66-GF30 30% Glass Reinforced, Heat Stabilized |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-30 PA666-GF30 Product description: Grilon TSG-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30 has the following important properties: Excellent fl.. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-30/4 FA PA666-GF30 Information provided by EMS Grivory |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-30/4 PA666-GF30 Product description: Grilon TSG-30/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30/4 has the following important properties: Good flo.. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-30/4 W PA666-GF30 Product description: Grilon TSG-30/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de.. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | dry; DIN 53 457 |
Hippe PA 66 GF 30 Nylon 66 30% Glass fiber Reinforced These polyamide components being reinforced with glass fiber up to 30% are not only highly wear-resistant, but also show high mechanical strength, stiffness and dimensional stability. They can also.. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 3021GH30 BK629 PA66-GF30 30% Glass Reinforced, Heat Stabilized |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | ISO 527-1/-2 |
Polyplastic Armamid® PA6 GF 30 HS-901 Nylon, 30% Glass Filled Injection molding, heat stabilizedInformation provided by PolyPlastic Group. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | |
LATI Latilub 75/4-05T G/30-V0 PBT, 30% Glass Fiber Reinforced, PTFE Filled, Flame Retardant Self-lubricating product based on Polybutylene Terephthalate (PBT). PTFE. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Afri.. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 73G45L NC010 Nylon 6
(Unverified Data**) 45% Glass Reinforced Polyamide 6Zytel 73G45L NC010 is a 45% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |