Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.50 GPa | 1090 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 SGF 30 Polyamide 6, 30% Milled Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 30% of milled glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consum.. |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | ASTM D638 |
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Tensile Modulus | 7.50 GPa @Temperature 23.0 °C |
1090 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ A700 G20 U-SO Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 GF 15 FRA 5 Polyamide 6, 15% Glass Fiber, Halogen Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,.. |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | 1 mm/min; ISO 527 - 1/2 |
Hexion Bakelite™ PF 31 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress, UL listed molding compound 1.5 mm/V-1 (All), 3 mm/V-0 (All), standardized molding compound.Applicat.. |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | 1 mm/min; ISO 527 - 1/2 |
Hexion Bakelite™ X30 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, reinforced with cotton and sisal fibers, increased notched impact strength.Application areas: Covers for electrical and electromagnetic devices.Information provided by Bak.. |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® AKV 35 H2.0 SR1 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, improved surface finishInformation provided by LANXESS. |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527-1,-2 |
Lanxess Durethan® BKV 325 Z H2.0 901510 Nylon 6, 25% Glass Fibers PA 6, 25% glass fibers, blow molding, impact modified, heat-ageing stabilized |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527-1/-2 |
Lanxess Pocan® C 3230 XF 000000 PBT + PC, 30% Glass Fiber PBT+PC, 30% glass fibers, injection molding, improved flowability, low tendency to warp, improved surface finish |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | ASTM-D790 |
Polyram PlusTek RD302G6 Nylon 12, 30% Glass Fiber 30% glass-fiber reinforced polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | ASTM D638 |
Plenco 7523 Phenolic, Granular, Transfer Molded PLENCO 07523 is a woodflour and cotton flock filled novolac phenolic molding compound, formulated for high impact industrial uses. UL recognized under component file E40654.Information supplied by P.. |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527-1/-2 |
Covestro Bayblend® T88 GF-20* Polycarbonate + SAN Glass Filled Impact Grade Developmental productInjection molding grade20 % GFoptimized heat ageing- and UV-stabilityvery good flowtensile modulus = 7500 MPaVicat/B 120 = 130 °CPreprocessingMax. Water content |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527-1/-2 |
DSM Akulon® K224-G4U (Dry) 23% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527-1/-2 |
DSM Akulon® S223-G6 Nylon 66-30% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527-1/-2 |
DSM Akulon® S223-HG6 Nylon 66-30% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | cond; ISO 527-1/-2 |
DSM Stanyl® 46SF5030 PA46-GF30 FR(17) 30% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 MX 400 CP Combination Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LBV-30H FWA black 9225 PA12-GF30 Product Description: Grilamid LBV-30H FWA black 9225 is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined wit.. |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527 |
Eurotec® Tecomid® NB40 GR15 NL XA70 PA6, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LBV-30H FWA nat PA12-GF30 Product Description: Grilamid LBV-30H FWA natural is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h.. |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Minlon® IG38C1 BK434 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon IG38C1 BK434 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527 |
Eurotec® Tecomid® NA40 GR15 NL XA 20 PA 6.6 15% glass fiber reinforced, UL94 V0 Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | ISO 527-1/-2 |
DSM Akulon® K-FHGM24 (Dry) 30% Glass/Mineral Reinforced, Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | STN EN ISO 527-2 |
Plastcom SLOVALEN PH 69 GF 30/1M Polypropylene reinforced with glass fiber Modified homopolymer PP for injection molding, reinforced with 30% glass fiber. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Pl.. |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON OE002 PPS - LINEAR LNP* STAT-KON* OE002 is a compound based on PPS - Linear resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | 1 mm/min |
Arkema Group Orgalloy® RS 6030 Nylon 6 Alloy, 30% Glass Fiber (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |
|||
Tensile Modulus | 7.50 GPa | 1090 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® DP AKV 35 LT H2.0 904040 Nylon 66, 35% Glass Fiber PA 66, injection molding grade, 35% glass fibers, black colored for laser transmission- welding (laser-transparent), good heat-ageing resistance |
|||
Tensile Modulus | 7.50 GPa @Temperature 23.0 °C |
1090 ksi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F.. |